CN105666060A - 一种汽车金属件冲压工艺 - Google Patents
一种汽车金属件冲压工艺 Download PDFInfo
- Publication number
- CN105666060A CN105666060A CN201610145406.8A CN201610145406A CN105666060A CN 105666060 A CN105666060 A CN 105666060A CN 201610145406 A CN201610145406 A CN 201610145406A CN 105666060 A CN105666060 A CN 105666060A
- Authority
- CN
- China
- Prior art keywords
- metal
- sheet
- metal plate
- washing
- automotive
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
本发明涉及汽车零部件制备领域,具体涉及一种汽车金属件冲压工艺,包括如下步骤:固定金属板的对角线两端,并沿对角线两端沿相反方向拉伸金属板,同时加热金属板使其体积膨胀;将金属板在折弯线位置进行折弯,且在折弯线位置电镀一层耐磨金属材料层;将金属板的边缘通过冲压去除毛刺;洗涤金属板,洗涤的溶液的组成为:硫酸镁2%、酚醛树脂20%的水溶液,其中百分比为质量分数;对洗涤后的金属板进行表面抛光处理。本发明采用的冲压工艺,拉伸效果好,而且对金属板进行洗涤时不对金属板造成腐蚀,且洗去有机物质,洗涤后不经清洗直接可用于抛光,即便洗涤液中成分附着于金属板表面也不影响其性能,相反的,酚醛树脂还提高了耐高温性能。
Description
技术领域
本发明涉及汽车零部件制备领域,具体涉及一种汽车金属件冲压工艺。
背景技术
汽车金属件的冲压过程中,拉伸比较困难,而且一般不经过洗涤就进行抛光处理,会在金属件表面留有杂质。
发明内容
为解决现有技术的问题,本发明的目的在于提供一种提高硬度、提高耐磨性能的汽车刹车片的制备方法。
为了实现上述目标,本发明采用如下的技术方案:一种汽车金属件冲压工艺,包括如下步骤:
(1)固定金属板的对角线两端,并沿对角线两端沿相反方向拉伸金属板,同时加热金属板使其体积膨胀;
(2)将步骤(1)得到的金属板在折弯线位置进行折弯,且在折弯线位置电镀一层耐磨金属材料层;折弯线位置为预设;
(3)将步骤(2)得到的金属板的边缘通过冲压去除毛刺;
(4)洗涤金属板,洗涤的溶液的组成为:硫酸镁2%、酚醛树脂20%的水溶液,其中百分比为质量分数;
(5)对洗涤后的金属板进行表面抛光处理。
在步骤(1)中,加热金属板的方式为,将金属板放置在锅炉盖上,所述的锅炉盖设有若干通孔,锅炉内放置沸水。
所述的耐磨金属材料层为铬,厚度为1-2mm。
所述的洗涤金属板具体步骤为:将金属板放置在洗涤溶液中静置1-2h。
所述的金属板的边缘是指金属板的所有边缘。
所述的洗涤金属板具体步骤为:将金属板放置在洗涤溶液中且在室温下静置1-2h。
本发明采用的冲压工艺,拉伸效果好,而且对金属板进行洗涤时不对金属板造成腐蚀,且洗去有机物质,洗涤后不经清洗直接可用于抛光,即便洗涤液中成分附着于金属板表面也不影响其性能,相反的,酚醛树脂还提高了耐高温性能。
具体实施方式
以下结合具体实施例对本发明作具体的介绍。
一种汽车金属件冲压工艺,包括如下步骤:
固定金属板的对角线两端,并沿对角线两端沿相反方向拉伸金属板,同时加热金属板使其体积膨胀;
将金属板在折弯线位置进行折弯,且在折弯线位置电镀一层耐磨金属材料层;折弯线位置为预设;
将金属板的边缘通过冲压去除毛刺;
洗涤金属板,洗涤的溶液的组成为:硫酸镁2%、酚醛树脂20%的水溶液,其中百分比为质量分数;
对洗涤后的金属板进行表面抛光处理。
加热金属板的方式为,将金属板放置在锅炉盖上,所述的锅炉盖设有若干通孔,锅炉内放置沸水。所述的耐磨金属材料层为铬,厚度为1-2mm。所述的洗涤金属板具体步骤为:将金属板放置在洗涤溶液中室温下静置1-2h。所述的金属板的边缘是指金属板的所有边缘。
需要说明的是,上述实施例不以任何形式限制本发明,凡采用等同替换或等效变换的方式所获得的技术方案,均落在本发明的保护范围内。
Claims (6)
1.一种汽车金属件冲压工艺,包括如下步骤:
(1)固定金属板的对角线两端,并沿对角线两端沿相反方向拉伸金属板,同时加热金属板使其体积膨胀;
(2)将步骤(1)得到的金属板在折弯线位置进行折弯,且在折弯线位置电镀一层耐磨金属材料层;
(3)将步骤(2)得到的金属板的边缘通过冲压去除毛刺;
(4)洗涤金属板,洗涤的溶液的组成为:硫酸镁2%、酚醛树脂20%的水溶液,其中百分比为质量分数;
(5)对洗涤后的金属板进行表面抛光处理。
2.根据权利要求1所述的一种汽车金属件冲压工艺,其特征在于,在步骤(1)中,加热金属板的方式为,将金属板放置在锅炉盖上,所述的锅炉盖设有若干通孔,锅炉内放置沸水。
3.根据权利要求1所述的一种汽车金属件冲压工艺,其特征在于,所述的耐磨金属材料层为铬,厚度为1-2mm。
4.根据权利要求1所述的一种汽车金属件冲压工艺,其特征在于,所述的洗涤金属板具体步骤为:将金属板放置在洗涤溶液中静置1-2h。
5.根据权利要求1所述的一种汽车金属件冲压工艺,其特征在于,所述的金属板的边缘是指金属板的所有边缘。
6.根据权利要求1所述的一种汽车金属件冲压工艺,其特征在于,所述的洗涤金属板具体步骤为:将金属板放置在洗涤溶液中且在室温下静置1-2h。