CN105525335A - 电腐蚀打标液及其制备方法 - Google Patents

电腐蚀打标液及其制备方法 Download PDF

Info

Publication number
CN105525335A
CN105525335A CN201610069448.8A CN201610069448A CN105525335A CN 105525335 A CN105525335 A CN 105525335A CN 201610069448 A CN201610069448 A CN 201610069448A CN 105525335 A CN105525335 A CN 105525335A
Authority
CN
China
Prior art keywords
electro
preparation
electrocorrosion
marking liquid
corrosion marking
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201610069448.8A
Other languages
English (en)
Inventor
杨家平
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Label (wuxi) Electronics Co Ltd
Original Assignee
Label (wuxi) Electronics Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Label (wuxi) Electronics Co Ltd filed Critical Label (wuxi) Electronics Co Ltd
Priority to CN201610069448.8A priority Critical patent/CN105525335A/zh
Publication of CN105525335A publication Critical patent/CN105525335A/zh
Pending legal-status Critical Current

Abstract

本发明涉及一种电腐蚀打标液及其制备方法,该电腐蚀打标液包括以下重量百分含量的组分:亚硝酸钠1-2%,柠檬酸酸三钠0.5-1%,硝酸钠0.1-0.5%,焦磷酸钾1-5%,氯化铵0.5-1%,硫尿0.1-0.5%,柠檬酸0.2-1.5%,丙三醇1-10%,蒸馏水83.5-90.6%,本发明提出的电腐蚀打标液,可以减少电腐蚀打标加工工艺中的缺陷,而且成本低廉,将其用于金属电印机在金属表面蚀刻文字、图案、速度快,清晰,环保,无异味,而且制备方法简单,易于推广。

Description

电腐蚀打标液及其制备方法
技术领域
本发明涉及一种电腐蚀打标液及其制备方法。
背景技术
目前国内外不锈钢、碳钢、铜材和铝材等一些金属制品的表面图案处理的方式主要包括:电腐蚀打标、激光打标、贴标签、丝网印刷等等。其中,电腐蚀打标利用的是“低电压在打标液的作用下使金属表面局部离子化”的高科技,可在各种金属上打印发黑或发白的“商标、产品名称、技术指标”等任何标识,具有机械操作简单、价格低廉的特点。
在电腐蚀打标工艺中,打标液是产品最终加工效果的关键影响因素,现有打标液存在的问题是,性质不稳定,会导致产品有缺陷,而且价格较高,增加了产品的生产成本。
有鉴于上述的缺陷,本设计人,积极加以研究创新,以期创设一种电腐蚀打标液及其制备方法,使其更具有产业上的利用价值。
发明内容
为解决上述技术问题,本发明的目的是提供一种电腐蚀打标液及其制备方法,可以减少电腐蚀打标加工工艺中的缺陷,而且成本低廉。
本发明提出的一种电腐蚀打标液,包括以下重量百分含量的组分:
本发明还提出了电腐蚀打标液的制备方法,包括以下步骤:常温下,在蒸馏水中依次加入各个组分,搅拌30分钟,溶解即可。
借由上述方案,本发明至少具有以下优点:本发明提出的电腐蚀打标液,可以减少电腐蚀打标加工工艺中的缺陷,而且成本低廉,将其用于金属电印机在金属表面蚀刻文字、图案、速度快,清晰,环保,无异味,而且制备方法简单,易于推广。
上述说明仅是本发明技术方案的概述,为了能够更清楚了解本发明的技术手段,并可依照说明书的内容予以实施,以下以本发明的较佳实施例详细说明如后。
具体实施方式
下面结合实施例,对本发明的具体实施方式作进一步详细描述。以下实施例用于说明本发明,但不用来限制本发明的范围。
实施例1
本发明提出的一种电腐蚀打标液,包括以下重量百分含量的组分:
电腐蚀打标液的制备方法,包括以下步骤:常温下,在蒸馏水中依次加入各个组分,搅拌30分钟,溶解即可。
实施例2
本发明提出的一种电腐蚀打标液,包括以下重量百分含量的组分:
电腐蚀打标液的制备方法,包括以下步骤:常温下,在蒸馏水中依次加入各个组分,搅拌30分钟,溶解即可。
实施例3
本发明提出的一种电腐蚀打标液,包括以下重量百分含量的组分:
电腐蚀打标液的制备方法,包括以下步骤:常温下,在蒸馏水中依次加入各个组分,搅拌30分钟,溶解即可。
综上所述,本发明提出的电腐蚀打标液,可以减少电腐蚀打标加工工艺中的缺陷,而且成本低廉,将其用于金属电印机在金属表面蚀刻文字、图案、速度快,清晰,环保,无异味,而且制备方法简单,易于推广。
以上所述仅是本发明的优选实施方式,并不用于限制本发明,应当指出,对于本技术领域的普通技术人员来说,在不脱离本发明技术原理的前提下,还可以做出若干改进和变型,这些改进和变型也应视为本发明的保护范围。

Claims (2)

1.一种电腐蚀打标液,其特征在于:包括以下重量百分含量的组分:
2.根据权利要求1所述的电腐蚀打标液的制备方法,其特征在于:包括以下步骤:常温下,在蒸馏水中依次加入各个组分,搅拌30分钟,溶解即可。
CN201610069448.8A 2016-02-01 2016-02-01 电腐蚀打标液及其制备方法 Pending CN105525335A (zh)