CN105330418A - Smart preparation system and method of slow-release microcrystallization metal salt mineral powder - Google Patents

Smart preparation system and method of slow-release microcrystallization metal salt mineral powder Download PDF

Info

Publication number
CN105330418A
CN105330418A CN201510768155.4A CN201510768155A CN105330418A CN 105330418 A CN105330418 A CN 105330418A CN 201510768155 A CN201510768155 A CN 201510768155A CN 105330418 A CN105330418 A CN 105330418A
Authority
CN
China
Prior art keywords
module
executive signal
raw material
unit
scheduled time
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510768155.4A
Other languages
Chinese (zh)
Inventor
卢晔
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Chengdu Jiushidu Industrial Product Design Co Ltd
Original Assignee
Chengdu Jiushidu Industrial Product Design Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Chengdu Jiushidu Industrial Product Design Co Ltd filed Critical Chengdu Jiushidu Industrial Product Design Co Ltd
Priority to CN201510768155.4A priority Critical patent/CN105330418A/en
Publication of CN105330418A publication Critical patent/CN105330418A/en
Pending legal-status Critical Current

Abstract

The invention discloses a smart preparation system and method of slow-release microcrystallization metal salt mineral powder. The smart preparation system comprises a heating module, a vibration module, a grinding module, a prompt module, a stirring module, a concentration module, a cooling module, a drying module, a PLC, a crushing module and a sensing module. The sensing module is used for sensing whether the raw material feeding amount reaches a certain preset value or not; the PLC controls the heating module, the prompt module, the vibration module, the grinding module, the stirring module, the concentration module, the cooling module, the drying module and the crushing module to execute related operation after internal analysis and calculation according to all sensing values. According to the smart preparation system and method of slow-release microcrystallization metal salt mineral powder, through accurate control over all parameters, the stability of the slow-release microcrystallization metal salt mineral powder can be effectively improved, and the releasing speed of the slow-release microcrystallization metal salt mineral powder after being applied to soil is reduced; the smart preparation system and method have high production efficiency, meet the production tact, lower labor intensity and are accurate and reliable in detection; the preparation efficiency can be effectively improved, the automated degree is high, operation is convenient, and resources are saved.

Description

A kind of slowly-releasing micritization metal-salt breeze intelligence preparation system and method
Technical field
The present invention relates to automation field, especially a kind of slowly-releasing micritization metal-salt breeze intelligence preparation system and method.
Background technology
The output of input to farm crop of fertilizer serves vital effect, but in the actual planting process of farm crop, long-term existence the problem of apply fertilizer single and excessive fertilization, and the average utilization of fertilizer is very low, and its major cause is the quick-acting of fertilizer and volatile fugitive volatile.The measure that correspondence is taked is then use release-controlled coated fertilizer to improve the utilization ratio of nutrient, but individual layer bag film strength is low, and slowly-releasing nutrients ratio is fixed, and without specific aim, the demand etc. of nutrient is constrained to the development of self.
Meanwhile, in the preparation process of fertilizer, a kind of slowly-releasing micritization metal-salt breeze plays vital effect, directly affects quality and the nutrient of fertilizer; The micro-stability of present stage is low, and after being manured into soil, dissolve rapidly and enter in soil, release rate is fast, makes a kind of utilization ratio of slowly-releasing micritization metal-salt breeze composting low.Because a kind of slowly-releasing micritization metal-salt breeze is as the important source material manufacturing fertilizer, need to produce in enormous quantities, at present, the preparation most due to a kind of slowly-releasing micritization metal-salt breeze relies on manual operation, and efficiency is low, at the bottom of level of automation, thus inconvenience is brought to operation, and comparatively waste resource.
Summary of the invention
Goal of the invention of the present invention is: for above-mentioned Problems existing, a kind of high efficiency is provided, meets productive temp, reduce labour intensity, detect a kind of slowly-releasing micritization metal-salt breeze intelligence preparation system and method accurately and reliably, by the accurate control to parameters, effectively can improve a kind of stability of slowly-releasing micritization metal-salt breeze, reduce its be manured into soil in release rate, effectively improve preparation efficiency, level of automation is high, easy to operate, save resource;
The technical solution used in the present invention is as follows:
A kind of slowly-releasing micritization metal-salt breeze intelligence preparation system; it is characterized in that, it comprises: heating module, vibration module, grinding module, reminding module, stirring module, concentrated module, refrigerating module, irradiation modules, PLC, pulverizing module and induction module;
Induction module comprises is located at heating unit two, the inductor block of whipping appts five, vibro-grinding device, concentrating unit, refrigerating unit and drying and crushing device; Described heating unit two, whipping appts five, vibro-grinding device, concentrating unit, refrigerating unit and drying and crushing device are provided with upper end open and lower ending opening; Described lower ending opening is provided with opening and closing valve; In heating unit two, when raw material adds weight >=preset value 0001, to PLC transmitting digital signals 0001; In whipping appts five, when raw material adds weight >=preset value 0002, to PLC transmitting digital signals 0002; In vibro-grinding device, when raw material adds weight >=preset value 0003, to PLC transmitting digital signals 0003; In concentrating unit, when raw material adds weight >=preset value 0004, to PLC transmitting digital signals 0004; In refrigerating unit, when raw material adds weight >=preset value 0005, to PLC transmitting digital signals 0005; In drying and crushing device, when raw material adds weight >=preset value 0006, to PLC transmitting digital signals 0006;
Described PLC is connected with induction module with heating module, reminding module, vibration module, grinding module, stirring module, concentrated module, refrigerating module, irradiation modules, pulverizing module respectively; For receiving digital signaling zero 001, transmit executive signal 1001 to heating module; Receive digital signaling zero 002, transmit executive signal 2001 to stirring module; Receive digital signaling zero 003, transmit executive signal 3001 to vibration module, transmit executive signal 4001 to grinding module simultaneously; Receive digital signaling zero 004, transmit executive signal 6001 to concentrated module; Receive digital signaling zero 005, transmit executive signal 7001 to refrigerating module; Receive digital signaling zero 006, transmit executive signal 8001 to irradiation modules, transmit executive signal 9001 to pulverizing module simultaneously; Receive digital signaling zero 007, transmit executive signal 5001 to reminding module;
Described heating module comprises heating unit two, for receiving executive signal 1001, starting heating unit two, switching to holding mode after heating water to preset temperature 0001;
Described stirring module comprises whipping appts five, and described whipping appts five is connected with heating unit two, for receiving executive signal 2001, starting whipping appts five scheduled time 0001, opening its opening and closing valve after completing;
Vibration module involving vibrations device, for receiving executive signal 3001, the Vibration on Start-up device scheduled time 0002;
Grinding module comprises milling apparatus, for receiving executive signal 4001, and the Vibration on Start-up milling apparatus scheduled time 0002; Complete backward PLC transmitting digital signals 0007;
Reminding module comprises warning howler, for receiving executive signal 5001, starting warning howler, sending prompt tone;
Concentrated module comprises concentrating unit, for receiving executive signal 6001, starting concentrating unit, being concentrated by raw material, stop, opening its opening and closing valve after completing after the scheduled time 0003;
Refrigerating module comprises refrigerating unit, for receiving executive signal 7001, opens its opening and closing valve after after the scheduled time 0004;
Irradiation modules comprises drying installation, for receiving executive signal 8001, starting drying installation, raw material is carried out drying, stop after the scheduled time 0005;
Pulverize module and comprise shredding unit, for receiving executive signal 9001, starting shredding unit, raw material is pulverized, stop after the scheduled time 0006;
Owing to adopting such scheme, described induction module adopts highly sensitive sensitive device, when its sense raw material add weight reach a certain preset value time, to PLC transmitting digital signals, PLC, after internal analysis, controls corresponding module and performs corresponding operation.Whole process automation degree is high, greatly saves man power and material.
Further, described whipping appts can be located in heating unit two, also can set up separately.
Owing to adopting such scheme, if whipping appts is located in heating unit two, then, when solution is heated to boiling, the agitator in whipping appts directly stirs in heating unit two; If whipping appts is set up separately, then, after solution is heated to boiling by heating unit two, solution is placed in whipping appts and stirs again.Two sets of plan adds the range of choice of user, can need to select any one mode according to self.
Further, described refrigerating unit floor space >10m2; And there are some ventilation openings side.
The present invention adopts the mode of naturally cooling to be cooled by raw material, because naturally cooling mode can better retain the nutrient of slowly-releasing micritization metal-salt breeze; In order to save cooling time, setting up enough large by the area of refrigerating unit, making its thickness in device thinner, cooling is faster, sets up some ventilation openings in the side of refrigerating unit simultaneously, accelerates speed of cooling.
Further, a kind of intelligent preparation method of slowly-releasing micritization metal-salt breeze intelligence preparation system, it is characterized in that, it comprises the following steps:
Step 1: install ready by each device, opens the power supply of a kind of slowly-releasing micritization metal-salt breeze intelligence preparation system;
Step 2: the water of pre-determined volume is added heating unit two, when the water is boiling, adds the agar of predetermined dose 0001 in heating unit two; In heating unit two, when induction module senses that raw material adds weight >=preset value 0001, to PLC transmitting digital signals 0001; PLC receives digital signaling zero 001, transmits executive signal 1001 to heating module; Heating module receives executive signal 1001, starts heating unit two, switches to holding mode after heating water to preset temperature 0001;
Step 3: when induction module senses that raw material adds weight >=preset value 0002 in whipping appts five, to PLC transmitting digital signals 0002; Receive digital signaling zero 002, transmit executive signal 2001 to stirring module; Described stirring module receives executive signal 2001, starts whipping appts five scheduled time 0001, opens its opening and closing valve after completing;
Step 4: the peroxophosphoric acid metal-salt of the dithiocarbamates of the azide metal salt of predetermined dose 0002, predetermined dose 0003, the selenous acid metal-salt of predetermined dose 0004 and predetermined dose 0005 is put into vibro-grinding device, when in vibro-grinding device, induction module senses that raw material adds weight >=preset value 0003, to PLC transmitting digital signals 0003; Receive digital signaling zero 003, transmit executive signal 3001 to vibration module, transmit executive signal 4001 to grinding module simultaneously, transmit executive signal 5001 to reminding module; Vibration module receives executive signal 3001, the Vibration on Start-up device scheduled time 0002; Grinding module receives executive signal 4001, starts the milling apparatus scheduled time 0002; Complete backward PLC transmitting digital signals 0007; Receive digital signaling zero 007, transmit executive signal 5002 to reminding module; Reminding module receives executive signal 5001, starts warning howler, sends prompt tone, and the micritization metal-salt after vibro-grinding is placed in micritization metal-salt collection device by prompting staff;
Step 5: the agar-agar soln in whipping appts five and the micritization metal-salt in micritization metal-salt collection device are placed in concentrating unit, induction module in concentrating unit senses when raw material adds weight >=preset value 0004, to PLC transmitting digital signals 0004; Receive digital signaling zero 004, transmit executive signal 6001 to concentrated module; Concentrated module receives executive signal 6001, starts concentrating unit, is concentrated by raw material, stops, opening its opening and closing valve after completing after the scheduled time 0003;
Step 6: raw material enters refrigerating unit, when in refrigerating unit, induction module senses that raw material adds weight >=preset value 0005, to PLC transmitting digital signals 0005; Receive digital signaling zero 005, transmit executive signal 7001 to refrigerating module; Refrigerating module receives executive signal 7001, is evenly laid on refrigerating unit by raw material, opens its opening and closing valve after the naturally cooling scheduled time 0004;
Step 7: raw material enters drying and crushing device, when in drying and crushing device, induction module senses that raw material adds weight >=preset value 0006, to PLC transmitting digital signals 0006; Receive digital signaling zero 006, transmit executive signal 8001 to irradiation modules, transmit executive signal 9001 to pulverizing module simultaneously; Irradiation modules receives executive signal 8001, starts drying installation, raw material is carried out drying, stops after the scheduled time 0005; Pulverize module and receive executive signal 9001, start shredding unit, raw material is pulverized, stop after the scheduled time 0006.
In sum, owing to have employed technique scheme, the invention has the beneficial effects as follows:
1, there is high efficiency, meet productive temp, reduce labour intensity, detect accurately and reliably;
2, by accurate control to parameters, effectively can improve a kind of stability of slowly-releasing micritization metal-salt breeze, reduce its be manured into soil in release rate;
3, effectively improve preparation efficiency, level of automation is high, easy to operate, saves resource.
Accompanying drawing explanation
Examples of the present invention will be described by way of reference to the accompanying drawings, wherein:
Fig. 1 is the schematic flow sheet of a kind of slowly-releasing micritization metal-salt breeze intelligence preparation system of the present invention.
Embodiment
All features disclosed in this specification sheets, or the step in disclosed all methods or process, except mutually exclusive feature and/or step, all can combine by any way.
Arbitrary feature disclosed in this specification sheets (comprising any accessory claim, summary), unless specifically stated otherwise, all can be replaced by other equivalences or the alternative features with similar object.That is, unless specifically stated otherwise, each feature is an example in a series of equivalence or similar characteristics.
As shown in Figure 1, a kind of slowly-releasing micritization metal-salt breeze intelligence preparation system, it comprises: heating module, vibration module, grinding module, reminding module, stirring module, concentrated module, refrigerating module, irradiation modules, PLC, pulverizing module and induction module;
Induction module comprises is located at heating unit two, the inductor block of whipping appts five, vibro-grinding device, concentrating unit, refrigerating unit and drying and crushing device; Described heating unit two, whipping appts five, vibro-grinding device, concentrating unit, refrigerating unit and drying and crushing device are provided with upper end open and lower ending opening; Described lower ending opening is provided with opening and closing valve; In heating unit two, when raw material adds weight >=preset value 0001, to PLC transmitting digital signals 0001; In whipping appts five, when raw material adds weight >=preset value 0002, to PLC transmitting digital signals 0002; In vibro-grinding device, when raw material adds weight >=preset value 0003, to PLC transmitting digital signals 0003; In concentrating unit, when raw material adds weight >=preset value 0004, to PLC transmitting digital signals 0004; In refrigerating unit, when raw material adds weight >=preset value 0005, to PLC transmitting digital signals 0005; In drying and crushing device, when raw material adds weight >=preset value 0006, to PLC transmitting digital signals 0006;
Described PLC is connected with induction module with heating module, reminding module, vibration module, grinding module, stirring module, concentrated module, refrigerating module, irradiation modules, pulverizing module respectively; For receiving digital signaling zero 001, transmit executive signal 1001 to heating module; Receive digital signaling zero 002, transmit executive signal 2001 to stirring module; Receive digital signaling zero 003, transmit executive signal 3001 to vibration module, transmit executive signal 4001 to grinding module simultaneously; Receive digital signaling zero 004, transmit executive signal 6001 to concentrated module; Receive digital signaling zero 005, transmit executive signal 7001 to refrigerating module; Receive digital signaling zero 006, transmit executive signal 8001 to irradiation modules, transmit executive signal 9001 to pulverizing module simultaneously; Receive digital signaling zero 007, transmit executive signal 5001 to reminding module;
Described heating module comprises heating unit two, for receiving executive signal 1001, starting heating unit two, switching to holding mode after heating water to preset temperature 0001;
Described stirring module comprises whipping appts five, and described whipping appts five is connected with heating unit two, for receiving executive signal 2001, starting whipping appts five scheduled time 0001, opening its opening and closing valve after completing;
Vibration module involving vibrations device, for receiving executive signal 3001, the Vibration on Start-up device scheduled time 0002;
Grinding module comprises milling apparatus, for receiving executive signal 4001, and the Vibration on Start-up milling apparatus scheduled time 0002; Complete backward PLC transmitting digital signals 0007;
Reminding module comprises warning howler, for receiving executive signal 5001, starting warning howler, sending prompt tone;
Concentrated module comprises concentrating unit, for receiving executive signal 6001, starting concentrating unit, being concentrated by raw material, stop, opening its opening and closing valve after completing after the scheduled time 0003;
Refrigerating module comprises refrigerating unit, for receiving executive signal 7001, opens its opening and closing valve after after the scheduled time 0004;
Irradiation modules comprises drying installation, for receiving executive signal 8001, starting drying installation, raw material is carried out drying, stop after the scheduled time 0005;
Pulverize module and comprise shredding unit, for receiving executive signal 9001, starting shredding unit, raw material is pulverized, stop after the scheduled time 0006;
Described whipping appts can be located in heating unit two, also can set up separately.
Described refrigerating unit floor space >10m2; And there are some ventilation openings side.
An intelligent preparation method for slowly-releasing micritization metal-salt breeze intelligence preparation system, it comprises the following steps:
Step 1: install ready by each device, opens the power supply of a kind of slowly-releasing micritization metal-salt breeze intelligence preparation system;
Step 2: the water of pre-determined volume is added heating unit two, when the water is boiling, adds the agar of predetermined dose 0001 in heating unit two; In heating unit two, when induction module senses that raw material adds weight >=preset value 0001, to PLC transmitting digital signals 0001; PLC receives digital signaling zero 001, transmits executive signal 1001 to heating module; Heating module receives executive signal 1001, starts heating unit two, switches to holding mode after heating water to preset temperature 0001;
Step 3: when induction module senses that raw material adds weight >=preset value 0002 in whipping appts five, to PLC transmitting digital signals 0002; Receive digital signaling zero 002, transmit executive signal 2001 to stirring module; Described stirring module receives executive signal 2001, starts whipping appts five scheduled time 0001, opens its opening and closing valve after completing;
Step 4: the peroxophosphoric acid metal-salt of the dithiocarbamates of the azide metal salt of predetermined dose 0002, predetermined dose 0003, the selenous acid metal-salt of predetermined dose 0004 and predetermined dose 0005 is put into vibro-grinding device, when in vibro-grinding device, induction module senses that raw material adds weight >=preset value 0003, to PLC transmitting digital signals 0003; Receive digital signaling zero 003, transmit executive signal 3001 to vibration module, transmit executive signal 4001 to grinding module simultaneously, transmit executive signal 5001 to reminding module; Vibration module receives executive signal 3001, the Vibration on Start-up device scheduled time 0002; Grinding module receives executive signal 4001, starts the milling apparatus scheduled time 0002; Complete backward PLC transmitting digital signals 0007; Receive digital signaling zero 007, transmit executive signal 5002 to reminding module; Reminding module receives executive signal 5001, starts warning howler, sends prompt tone, and the micritization metal-salt after vibro-grinding is placed in micritization metal-salt collection device by prompting staff;
Step 5: the agar-agar soln in whipping appts five and the micritization metal-salt in micritization metal-salt collection device are placed in concentrating unit, induction module in concentrating unit senses when raw material adds weight >=preset value 0004, to PLC transmitting digital signals 0004; Receive digital signaling zero 004, transmit executive signal 6001 to concentrated module; Concentrated module receives executive signal 6001, starts concentrating unit, is concentrated by raw material, stops, opening its opening and closing valve after completing after the scheduled time 0003;
Step 6: raw material enters refrigerating unit, when in refrigerating unit, induction module senses that raw material adds weight >=preset value 0005, to PLC transmitting digital signals 0005; Receive digital signaling zero 005, transmit executive signal 7001 to refrigerating module; Refrigerating module receives executive signal 7001, is evenly laid on refrigerating unit by raw material, opens its opening and closing valve after the naturally cooling scheduled time 0004;
Step 7: raw material enters drying and crushing device, when in drying and crushing device, induction module senses that raw material adds weight >=preset value 0006, to PLC transmitting digital signals 0006; Receive digital signaling zero 006, transmit executive signal 8001 to irradiation modules, transmit executive signal 9001 to pulverizing module simultaneously; Irradiation modules receives executive signal 8001, starts drying installation, raw material is carried out drying, stops after the scheduled time 0005; Pulverize module and receive executive signal 9001, start shredding unit, raw material is pulverized, stop after the scheduled time 0006.
A kind of whole preparation system of liquid sustained-controll-release fertiliser for improving soil metal salt concentration is as follows:
It comprises the slowly-releasing microorganism agent syntheti c route be in parallel, slowly releasing trace element sequestrant syntheti c route and slowly-releasing micritization metal-salt breeze syntheti c route, slowly-releasing microorganism agent syntheti c route, slowly releasing trace element sequestrant syntheti c route and slowly-releasing micritization metal-salt breeze syntheti c route cross and are connected to liquid sustained-controll-release fertiliser syntheti c route.
Slowly-releasing microorganism agent syntheti c route comprises the diatomite pre-treatment route and microbial pretreatment route that are in parallel, diatomite comprises with process route the diatomite entrance and milling apparatus that are linked in sequence, microbial pretreatment route comprises some microorganism entrances and syrup inking device, and some microorganism entrances and syrup inking device cross and be connected whipping appts one and suspension collection device; Diatomite pre-treatment route and microbial pretreatment route cross and are connected to whipping appts two, whipping appts two and organic carrier syntheti c route cross and are connected to whipping appts three, described organic carrier syntheti c route comprises cow dung entrance and straw entrance, described cow dung entrance and straw entrance cross and are connected to whipping appts four, whipping appts four connects organic carrier collection device, and whipping appts two and organic carrier collection device cross and be connected to whipping appts three; Whipping appts three is linked in sequence filtration unit and gas blower.It is 42% that syrup can be configured to concentration by syrup inking device; It is 325 orders that diatomite can be ground to form fineness by milling apparatus; The number of microorganism entrance is 4, is respectively filamentous bacterium entrance, phosphorus decomposing bacillus megaterium entrance, bacillusmusilaginosiengineering entrance and photosynthetic bacteria entrance; Filamentous bacterium entrance, phosphorus decomposing bacillus megaterium entrance, bacillusmusilaginosiengineering entrance, photosynthetic bacteria entrance, diatomite entrance, cow dung entrance, straw entrance syrup inking device is all provided with weighing device; It is 38 DEG C that whipping appts four is placed in temperature, and degree of ventilation is under the environment of 22CBM/h; Gas blower is provided with thermostat, can be 28 DEG C by homo(io)thermism.By filamentous bacterium, phosphorus decomposing bacillus megaterium, gel-shaped bacillus, it is in the syrup of 42% that photosynthetic bacteria adds concentration, and stir to obtain microorganism suspension; By cow dung and plant straw Homogeneous phase mixing, be under the condition of 38 DEG C in temperature, degree of ventilation is 22CBM/h, compost 9day, obtained organic carrier; Diatomite being ground to fineness is 325 orders, is added in microorganism suspension by the diatomite after grinding, stirs; The microorganism suspension liquid stirred and organic carrier are mixed in proportion, stir 40min, leach fine particle, at 28 DEG C, use gas blower air-dry.
Slowly releasing trace element sequestrant syntheti c route comprises the EDTA entrance and hydrochloric acid entrance that are in parallel, EDTA entrance crosses with hydrochloric acid entrance and is connected solvent collection device, solvent collection device is provided with Calcium hydrogen carbonate entrance, solvent collection device sequence connects filtration unit two, heating unit one, cooling and stirring device, drying installation and shredding unit, heating unit one is provided with some trace metal salts entrances, and cooling and stirring device is provided with wilkinite entrance.Solvent collection device is provided with pH proofing unit; The number of some trace metal salts entrances is 5, is respectively copper sulfate entrance, zinc sulfate entrance, sulfuric acid boron entrance, molybdenum trisulfate entrance and manganous sulfate entrance; EDTA entrance, copper sulfate entrance, zinc sulfate entrance, sulfuric acid boron entrance, molybdenum trisulfate entrance and manganous sulfate entrance are equipped with weighing device.EDTA is dissolved in hydrochloric acid, adds Calcium hydrogen carbonate and regulate pH to 4.8, filter; In filtrate, add copper sulfate, be heated to 70 DEG C, chelating 3h; Zinc sulfate is added in solution, under the condition of 75 DEG C, chelating 3h; Sulfuric acid boron is added in solution, under the condition of 80 DEG C, chelating 3h; Molybdenum trisulfate is added in solution, under the condition of 80 DEG C, chelating 3h; Manganous sulfate is added in solution, under the condition of 82 DEG C, chelating 3h; Added by wilkinite in gained chelating liquid, drying is also pulverized, and obtains slowly releasing trace element sequestrant.
Slowly-releasing micritization metal-salt breeze syntheti c route comprises the agar-agar soln syntheti c route and micritization metal-salt syntheti c route that are in parallel, and agar-agar soln syntheti c route and micritization metal-salt syntheti c route cross and be connected to mixing route; Agar-agar soln syntheti c route comprises the heating unit two and whipping appts five that are linked in sequence, heating unit two is provided with agar entrance, micritization metal-salt syntheti c route comprises the metal-salt entrance be linked in sequence, vibro-grinding device and micritization metal-salt collection device, mixing route comprises the concentrating unit be linked in sequence, refrigerating unit, drying and crushing device; Whipping appts five and micritization salt collection device cross and are connected to concentrating unit.Agar entrance and metal-salt entrance are equipped with weighing device, and concentrating unit is provided with agitator.By azide metal salt, dithiocarbamates, selenous acid metal-salt, peroxophosphoric acid metal-salt adopts vibration mill micronization to obtain micritization metal-salt; Get intermediate water and be heated to boiling, add agar, be stirred to agar under the state keeping boiling and dissolve completely; Mixed with agar-agar soln by micritization metal-salt, continuous heating is to thick, and drying after naturally cooling is also pulverized, and obtains slowly-releasing micritization metal mining powder.
Liquid sustained-controll-release fertiliser syntheti c route comprises the whipping appts six be linked in sequence, whipping appts seven, refrigerating unit two and finished product collection device, and whipping appts six is provided with heating unit, and whipping appts six is provided with washing water of rice entrance and ammonia inlet; Whipping appts seven and slowly-releasing microorganism agent syntheti c route, slowly releasing trace element sequestrant syntheti c route is connected with slowly-releasing micritization metal-salt breeze syntheti c route; Refrigerating unit two is provided with sodium alginate and chitosan entrance.Whipping appts six is provided with thermostat, can by homo(io)thermism at 24 DEG C; Refrigerating unit two is provided with thermostat, can by homo(io)thermism at 12 DEG C, and refrigerating unit two is provided with agitator; Washing water of rice entrance, ammonia inlet, sodium alginate entrance and chitosan entrance are equipped with weighing device.Washing water of rice and ammoniacal liquor are mixed, is heated to 24 DEG C; By slowly-releasing microorganism agent, slowly releasing trace element sequestrant and slowly-releasing micritization metal mining powder add in mixing solutions, stir; Be cooled to 12 DEG C, add sodium alginate and chitosan, stir.
The present invention is not limited to aforesaid embodiment.The present invention expands to any new feature of disclosing in this manual or any combination newly, and the step of the arbitrary new method disclosed or process or any combination newly.

Claims (4)

1. a slowly-releasing micritization metal-salt breeze intelligence preparation system; it is characterized in that, it comprises: heating module, vibration module, grinding module, reminding module, stirring module, concentrated module, refrigerating module, irradiation modules, PLC, pulverizing module and induction module;
Induction module comprises is located at heating unit two, the inductor block of whipping appts five, vibro-grinding device, concentrating unit, refrigerating unit and drying and crushing device; Described heating unit two, whipping appts five, vibro-grinding device, concentrating unit, refrigerating unit and drying and crushing device are provided with upper end open and lower ending opening; Described lower ending opening is provided with opening and closing valve; In heating unit two, when raw material adds weight >=preset value 0001, to PLC transmitting digital signals 0001; In whipping appts five, when raw material adds weight >=preset value 0002, to PLC transmitting digital signals 0002; In vibro-grinding device, when raw material adds weight >=preset value 0003, to PLC transmitting digital signals 0003; In concentrating unit, when raw material adds weight >=preset value 0004, to PLC transmitting digital signals 0004; In refrigerating unit, when raw material adds weight >=preset value 0005, to PLC transmitting digital signals 0005; In drying and crushing device, when raw material adds weight >=preset value 0006, to PLC transmitting digital signals 0006;
Described PLC is connected with induction module with heating module, reminding module, vibration module, grinding module, stirring module, concentrated module, refrigerating module, irradiation modules, pulverizing module respectively; For receiving digital signaling zero 001, transmit executive signal 1001 to heating module; Receive digital signaling zero 002, transmit executive signal 2001 to stirring module; Receive digital signaling zero 003, transmit executive signal 3001 to vibration module, transmit executive signal 4001 to grinding module simultaneously; Receive digital signaling zero 004, transmit executive signal 6001 to concentrated module; Receive digital signaling zero 005, transmit executive signal 7001 to refrigerating module; Receive digital signaling zero 006, transmit executive signal 8001 to irradiation modules, transmit executive signal 9001 to pulverizing module simultaneously; Receive digital signaling zero 007, transmit executive signal 5001 to reminding module;
Described heating module comprises heating unit two, for receiving executive signal 1001, starting heating unit two, switching to holding mode after heating water to preset temperature 0001;
Described stirring module comprises whipping appts five, and described whipping appts five is connected with heating unit two, for receiving executive signal 2001, starting whipping appts five scheduled time 0001, opening its opening and closing valve after completing;
Vibration module involving vibrations device, for receiving executive signal 3001, the Vibration on Start-up device scheduled time 0002;
Grinding module comprises milling apparatus, for receiving executive signal 4001, and the Vibration on Start-up milling apparatus scheduled time 0002; Complete backward PLC transmitting digital signals 0007;
Reminding module comprises warning howler, for receiving executive signal 5001, starting warning howler, sending prompt tone;
Concentrated module comprises concentrating unit, for receiving executive signal 6001, starting concentrating unit, being concentrated by raw material, stop, opening its opening and closing valve after completing after the scheduled time 0003;
Refrigerating module comprises refrigerating unit, for receiving executive signal 7001, opens its opening and closing valve after after the scheduled time 0004;
Irradiation modules comprises drying installation, for receiving executive signal 8001, starting drying installation, raw material is carried out drying, stop after the scheduled time 0005;
Pulverize module and comprise shredding unit, for receiving executive signal 9001, starting shredding unit, raw material is pulverized, stop after the scheduled time 0006.
2. a kind of slowly-releasing micritization metal-salt breeze intelligence preparation system as claimed in claim 1, it is characterized in that, described whipping appts can be located in heating unit two, also can set up separately.
3. a kind of slowly-releasing micritization metal-salt breeze intelligence preparation system as claimed in claim 2, is characterized in that, described refrigerating unit floor space >10m2; And there are some ventilation openings side.
4. the intelligent preparation method of a kind of slowly-releasing micritization metal-salt breeze intelligence preparation system as described in one of claims 1 to 3, it is characterized in that, it comprises the following steps:
Step 1: install ready by each device, opens the power supply of a kind of slowly-releasing micritization metal-salt breeze intelligence preparation system;
Step 2: the water of pre-determined volume is added heating unit two, when the water is boiling, adds the agar of predetermined dose 0001 in heating unit two; In heating unit two, when induction module senses that raw material adds weight >=preset value 0001, to PLC transmitting digital signals 0001; PLC receives digital signaling zero 001, transmits executive signal 1001 to heating module; Heating module receives executive signal 1001, starts heating unit two, switches to holding mode after heating water to preset temperature 0001;
Step 3: when induction module senses that raw material adds weight >=preset value 0002 in whipping appts five, to PLC transmitting digital signals 0002; Receive digital signaling zero 002, transmit executive signal 2001 to stirring module; Described stirring module receives executive signal 2001, starts whipping appts five scheduled time 0001, opens its opening and closing valve after completing;
Step 4: the peroxophosphoric acid metal-salt of the dithiocarbamates of the azide metal salt of predetermined dose 0002, predetermined dose 0003, the selenous acid metal-salt of predetermined dose 0004 and predetermined dose 0005 is put into vibro-grinding device, when in vibro-grinding device, induction module senses that raw material adds weight >=preset value 0003, to PLC transmitting digital signals 0003; Receive digital signaling zero 003, transmit executive signal 3001 to vibration module, transmit executive signal 4001 to grinding module simultaneously, transmit executive signal 5001 to reminding module; Vibration module receives executive signal 3001, the Vibration on Start-up device scheduled time 0002; Grinding module receives executive signal 4001, starts the milling apparatus scheduled time 0002; Complete backward PLC transmitting digital signals 0007; Receive digital signaling zero 007, transmit executive signal 5002 to reminding module; Reminding module receives executive signal 5001, starts warning howler, sends prompt tone, and the micritization metal-salt after vibro-grinding is placed in micritization metal-salt collection device by prompting staff;
Step 5: the agar-agar soln in whipping appts five and the micritization metal-salt in micritization metal-salt collection device are placed in concentrating unit, induction module in concentrating unit senses when raw material adds weight >=preset value 0004, to PLC transmitting digital signals 0004; Receive digital signaling zero 004, transmit executive signal 6001 to concentrated module; Concentrated module receives executive signal 6001, starts concentrating unit, is concentrated by raw material, stops, opening its opening and closing valve after completing after the scheduled time 0003;
Step 6: raw material enters refrigerating unit, when in refrigerating unit, induction module senses that raw material adds weight >=preset value 0005, to PLC transmitting digital signals 0005; Receive digital signaling zero 005, transmit executive signal 7001 to refrigerating module; Refrigerating module receives executive signal 7001, is evenly laid on refrigerating unit by raw material, opens its opening and closing valve after the naturally cooling scheduled time 0004;
Step 7: raw material enters drying and crushing device, when in drying and crushing device, induction module senses that raw material adds weight >=preset value 0006, to PLC transmitting digital signals 0006; Receive digital signaling zero 006, transmit executive signal 8001 to irradiation modules, transmit executive signal 9001 to pulverizing module simultaneously; Irradiation modules receives executive signal 8001, starts drying installation, raw material is carried out drying, stops after the scheduled time 0005; Pulverize module and receive executive signal 9001, start shredding unit, raw material is pulverized, stop after the scheduled time 0006.
CN201510768155.4A 2015-11-12 2015-11-12 Smart preparation system and method of slow-release microcrystallization metal salt mineral powder Pending CN105330418A (en)