CN105274700A - Processing technology of puff seersucker - Google Patents

Processing technology of puff seersucker Download PDF

Info

Publication number
CN105274700A
CN105274700A CN201410348162.4A CN201410348162A CN105274700A CN 105274700 A CN105274700 A CN 105274700A CN 201410348162 A CN201410348162 A CN 201410348162A CN 105274700 A CN105274700 A CN 105274700A
Authority
CN
China
Prior art keywords
seersucker
lantern
processing technology
puff
carry
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410348162.4A
Other languages
Chinese (zh)
Inventor
王沛龙
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Run Long Fabritex Srl Of Jurong City
Original Assignee
Run Long Fabritex Srl Of Jurong City
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Run Long Fabritex Srl Of Jurong City filed Critical Run Long Fabritex Srl Of Jurong City
Priority to CN201410348162.4A priority Critical patent/CN105274700A/en
Publication of CN105274700A publication Critical patent/CN105274700A/en
Pending legal-status Critical Current

Abstract

The invention discloses a processing technology of a puff seersucker. The puff seersucker comprises warps and wefts, wherein the warp comprises puff warps and ground warps, the puff warp is a non-elastic yarn, and the ground warps and the wefts are made of Iceland yarns wound by a single puff fur yarn. The processing technology of the puff seersucker comprises that (1) a puff seersucker gray fabric with the structure is pretreated; (2) the pretreated gray fabric is refined through refinement processes including tentering, printing and baking; and (3) the refined gray fabric is post-treated and made into a puff seersucker finished product, wherein the post-treating process is a softening process. By the processing technology of the puff seersucker disclosed by the invention, the puff seersucker with a lantern-shaped surface can be produced. The puff seersucker is nicer and very comfortable.

Description

A kind of processing technology of lantern seersucker
Technical field
The invention belongs to fabric technical field, relate to a kind of processing technology of seersucker, particularly relate to a kind of processing technology of lantern seersucker.
Background technology
Existing garment material is a lot, but due to the raising of people's living standard, more and more higher to the requirement of fabric, developing this needs the more new varieties of exploitation to remove the needs of satisfied different consumer.
Seersucker is deeply by a kind of garment material that consumer likes, because its moisture absorption is ventilative, elegant in appearance, is thus widely used in making the easy suits such as nightwear, jacket, shirt.
But the seersucker shape of existing manufacture technics is single, and comfort level still cannot be satisfied the demand.
Summary of the invention
Technical problem to be solved by this invention is, overcomes the shortcoming of prior art, provides a kind of processing technology of lantern seersucker, can produce the seersucker of surface for lantern-shaped, more attractive in appearance, and has higher comfort level.
In order to solve above technical problem, the invention provides a kind of processing technology of lantern seersucker, lantern seersucker comprises warp thread and weft yarn, and warp thread comprises bubble warp and ground warp, and bubble is through being non-elastic yarn, and ground warp and weft yarn adopt Iceland's hair being wound with single pine tag silk;
The processing technology of lantern seersucker comprises:
(1) carry out pre-treatment to the seersucker grey cloth of said structure, the mercerising time of the mercerizing process of pre-treatment is 42s, and the concentration of mercerising alkali lye is 268-273g/L, and pick-up rate is 113%, and mercerising temperature is 19 DEG C;
(2) carry out refining to the grey cloth after pre-treatment, refining procedure comprises: tentering, stamp and cure operation; Tentering operation is at room temperature carried out; Printing technology adopts foaming to print and distribute technique; Cure operation: stoving temperature is 185-196 DEG C, the time of curing is 1.5-1.8min;
(3) carry out post processing to the grey cloth after refining and make finished product seersucker, postprocessing working procedures is softening step, and the soak time of softening step is 20-25min, water temperature 35-45 DEG C.
The technical scheme that the present invention limits further is:
After aforementioned mercerizing process terminates, carry out lixiviating operation immediately, after lixiviating, then carry out subsequent handling, lixiviating operation is: use suction device by hot diluted alkaline drip washing fabric; After loosening weft tension, enter lixiviating case, steam with light alkali cleaning.
Aforementioned cure operation after also comprise pressing treatment process, the temperature of described pressing treatment process is 125-130 DEG C, and the time is 3-5s, and pressure is 9.4-9.8N.
After aforementioned softening step completes, Direct Dehydration is dried, and obtain finished product seersucker, wherein bake out temperature is 160-165 DEG C, and drying time is 2-2.3min.
The invention has the beneficial effects as follows:
The concentration of mercerising alkali lye of the present invention is 268-273g/L, due to lower than 250g/L, mercerization effect is very poor in other words then can not to produce mercerization, but as more than 300g/L, due to the relative thickness of solution, NaOH molecule just can not enter fibrous inside rapidly, can affect the uniformity of mercerization effect, the concentration that the present invention adopts can ensure that the uniformity of mercerization effect is good, and mercerization effect is good.
After mercerizing process of the present invention terminates, carry out lixiviating operation immediately, after lixiviating, then carry out subsequent handling, lixiviating operation is: use suction device by hot diluted alkaline drip washing fabric; After loosening weft tension, enter lixiviating case, steam with light alkali cleaning.Relative to general washing lixiviating method, lixiviating effect can be improved.
The present invention can produce the seersucker of surface for lantern-shaped, more attractive in appearance, and has higher comfort level.
Detailed description of the invention
embodiment 1
Present embodiments provide a kind of processing technology of lantern seersucker, lantern seersucker comprises warp thread and weft yarn, and warp thread comprises bubble warp and ground warp, and bubble is through being non-elastic yarn, and ground warp and weft yarn adopt Iceland's hair being wound with single pine tag silk;
The processing technology of lantern seersucker comprises:
(1) carry out pre-treatment to the seersucker grey cloth of said structure, the mercerising time of the mercerizing process of pre-treatment is 42s, and the concentration of mercerising alkali lye is 268g/L, and pick-up rate is 113%, and mercerising temperature is 19 DEG C; After mercerizing process terminates, carry out lixiviating operation immediately, after lixiviating, then carry out subsequent handling, lixiviating operation is: use suction device by hot diluted alkaline drip washing fabric; After loosening weft tension, enter lixiviating case, steam with light alkali cleaning.
(2) carry out refining to the grey cloth after pre-treatment, refining procedure comprises: tentering, stamp and cure operation; Tentering operation is at room temperature carried out; Printing technology adopts foaming to print and distribute technique; Cure operation: stoving temperature is 196 DEG C, the time of curing is 1.5min; Also comprise pressing treatment process after curing operation, the temperature of described pressing treatment process is 127 DEG C, and the time is 4s, and pressure is 9.4N.
(3) carry out post processing to the grey cloth after refining and make finished product seersucker, postprocessing working procedures is softening step, and the soak time of softening step is 23min, water temperature 45 DEG C.After softening step completes, Direct Dehydration is dried, and obtain finished product seersucker, wherein bake out temperature is 165 DEG C, and drying time is 2-2.2min.
embodiment 2
Present embodiments provide a kind of processing technology of lantern seersucker, lantern seersucker comprises warp thread and weft yarn, and warp thread comprises bubble warp and ground warp, and bubble is through being non-elastic yarn, and ground warp and weft yarn adopt Iceland's hair being wound with single pine tag silk;
The processing technology of lantern seersucker comprises:
(1) carry out pre-treatment to the seersucker grey cloth of said structure, the mercerising time of the mercerizing process of pre-treatment is 42s, and the concentration of mercerising alkali lye is 273g/L, and pick-up rate is 113%, and mercerising temperature is 19 DEG C; After mercerizing process terminates, carry out lixiviating operation immediately, after lixiviating, then carry out subsequent handling, lixiviating operation is: use suction device by hot diluted alkaline drip washing fabric; After loosening weft tension, enter lixiviating case, steam with light alkali cleaning.
(2) carry out refining to the grey cloth after pre-treatment, refining procedure comprises: tentering, stamp and cure operation; Tentering operation is at room temperature carried out; Printing technology adopts foaming to print and distribute technique; Cure operation: stoving temperature is 191 DEG C, the time of curing is 1.7min; Also comprise pressing treatment process after curing operation, the temperature of described pressing treatment process is 130 DEG C, and the time is 5s, and pressure is 9.8N.
(3) carry out post processing to the grey cloth after refining and make finished product seersucker, postprocessing working procedures is softening step, and the soak time of softening step is 25min, water temperature 35 DEG C.After softening step completes, Direct Dehydration is dried, and obtain finished product seersucker, wherein bake out temperature is 162 DEG C, and drying time is 2.3min.
embodiment 3
Present embodiments provide a kind of processing technology of lantern seersucker, lantern seersucker comprises warp thread and weft yarn, and warp thread comprises bubble warp and ground warp, and bubble is through being non-elastic yarn, and ground warp and weft yarn adopt Iceland's hair being wound with single pine tag silk;
The processing technology of lantern seersucker comprises:
(1) carry out pre-treatment to the seersucker grey cloth of said structure, the mercerising time of the mercerizing process of pre-treatment is 42s, and the concentration of mercerising alkali lye is 271g/L, and pick-up rate is 113%, and mercerising temperature is 19 DEG C; After mercerizing process terminates, carry out lixiviating operation immediately, after lixiviating, then carry out subsequent handling, lixiviating operation is: use suction device by hot diluted alkaline drip washing fabric; After loosening weft tension, enter lixiviating case, steam with light alkali cleaning.
(2) carry out refining to the grey cloth after pre-treatment, refining procedure comprises: tentering, stamp and cure operation; Tentering operation is at room temperature carried out; Printing technology adopts foaming to print and distribute technique; Cure operation: stoving temperature is 185 DEG C, the time of curing is 1.5min; Also comprise pressing treatment process after curing operation, the temperature of described pressing treatment process is 125 DEG C, and the time is 3s, and pressure is 9.5N.
(3) carry out post processing to the grey cloth after refining and make finished product seersucker, postprocessing working procedures is softening step, and the soak time of softening step is 20min, water temperature 37 DEG C.After softening step completes, Direct Dehydration is dried, and obtain finished product seersucker, wherein bake out temperature is 160 DEG C, and drying time is 2min.
In addition to the implementation, the present invention can also have other embodiments, and all employings are equal to the technical scheme of replacement or equivalent transformation formation, all drop on the protection domain of application claims.

Claims (4)

1. a processing technology for lantern seersucker, is characterized in that:
Described lantern seersucker comprises warp thread and weft yarn, and described warp thread comprises bubble warp and ground warp, and described bubble is through being non-elastic yarn, and described ground warp and weft yarn adopt Iceland's hair being wound with single pine tag silk;
The processing technology of described lantern seersucker comprises:
Carry out pre-treatment to the seersucker grey cloth of said structure, the mercerising time of the mercerizing process of described pre-treatment is 42s, and the concentration of mercerising alkali lye is 268-273g/L, and pick-up rate is 113%, and mercerising temperature is 19 DEG C;
Carry out refining to the grey cloth after described pre-treatment, described refining procedure comprises: tentering, stamp and cure operation; Described tentering operation is at room temperature carried out; Described printing technology adopts foaming to print and distribute technique; Describedly cure operation: stoving temperature is 185-196 DEG C, and the time of curing is 1.5-1.8min;
Carry out post processing to the grey cloth after described refining and make finished product seersucker, described postprocessing working procedures is softening step, and the soak time of described softening step is 20-25min, water temperature 35-45 DEG C.
2. according to the processing technology of the lantern seersucker described in claim 1, it is characterized in that: after described mercerizing process terminates, carry out lixiviating operation immediately, after lixiviating, carry out subsequent handling again, described lixiviating operation is: use suction device by hot diluted alkaline drip washing fabric; After loosening weft tension, enter lixiviating case, steam with light alkali cleaning.
3., according to the processing technology of the lantern seersucker described in claim 1, it is characterized in that: described in cure operation after also comprise pressing treatment process, the temperature of described pressing treatment process is 125-130 DEG C, and the time is 3-5s, and pressure is 9.4-9.8N.
4. according to the processing technology of the lantern seersucker described in claim 1, it is characterized in that: after described softening step completes, Direct Dehydration is dried, and obtain finished product seersucker, wherein bake out temperature is 160-165 DEG C, and drying time is 2-2.3min.
CN201410348162.4A 2014-07-22 2014-07-22 Processing technology of puff seersucker Pending CN105274700A (en)