CN105128106A - 一种竹条改性用增韧保色浸泡液及其使用方法 - Google Patents

一种竹条改性用增韧保色浸泡液及其使用方法 Download PDF

Info

Publication number
CN105128106A
CN105128106A CN201510365613.XA CN201510365613A CN105128106A CN 105128106 A CN105128106 A CN 105128106A CN 201510365613 A CN201510365613 A CN 201510365613A CN 105128106 A CN105128106 A CN 105128106A
Authority
CN
China
Prior art keywords
parts
sodium
modification
soak
bamboo strip
Prior art date
Application number
CN201510365613.XA
Other languages
English (en)
Inventor
张大昌
Original Assignee
安徽昌发实业有限公司
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 安徽昌发实业有限公司 filed Critical 安徽昌发实业有限公司
Priority to CN201510365613.XA priority Critical patent/CN105128106A/zh
Publication of CN105128106A publication Critical patent/CN105128106A/zh

Abstract

本发明涉及编织工艺品用材料改性处理领域,具体涉及一种竹条改性用增韧保色浸泡液及其使用方法,其组成原料的重量份为:硫酸锌3-5、脂肪醇聚氧乙烯醚硫酸钠4-5、石油磺酸钠2-4、白果2-4、过氧碳酸钠6-9、钼酸钠5-8、尿素15-18、水250-280、助剂4-5;本发明制备的浸泡液不含挥发性毒性有机物成分,原料中的硫酸锌、钼酸钠、尿素、过氧碳酸钠等成分能够有效的软化竹条,达到促渗、阻燃、防腐、保色等功效,白果水煎液能驱虫防蛀,提高竹条对外界微生物的抵御能力;本发明浸泡液改性后的竹条色泽明亮均匀,柔韧易塑,不易折断,生产效率获得提升,所得产品长时间不变色,不易霉腐虫蛀,阻燃安全,经久耐用。

Description

一种竹条改性用増韧保色浸泡液及其使用方法

技术领域

[0001] 本发明涉及编织工艺品用材料改性处理领域,具体涉及一种竹条改性用增韧保色浸泡液及其使用方法。

背景技术

[0002] 藤条、柳条、竹条、各类秸杆等天然编制材料制作的工艺品具有极高的观赏和实用价值,产品远销国内外,极受消费者喜爱,市场潜力巨大。由于它们的生物特质,存在易燃、易裂、易虫蛀腐烂等缺点,在实际使用过程中需要进行一系列的改性处理,以改善其力学性能和理化性质,使其更易加工和运输储存,提高观赏价值和实用性能,常用的处理手段是采用改性液对材料浸泡处理,因此,改性液的配制尤为重要,理想的改性液需要具备环保无毒、改性效果持久、不影响美观等特点。

发明内容

[0003] 本发明目的在于提供一种竹条改性用增韧保色浸泡液及其使用方法,改善竹条使用性能,增进实用价值,为了实现上述目的,本发明采用的技术方案如下:

一种竹条改性用增韧保色浸泡液及其使用方法,其特征在于,该浸泡液由以下重量份的原料制成:硫酸锌3-5、脂肪醇聚氧乙烯醚硫酸钠4-5、石油磺酸钠2-4、白果2-4、过氧碳酸钠6-9、钼酸钠5-8、尿素15-18、水250-280、助剂4-5 ;

助剂由以下重量份的原料制成:二氢月桂烯醇2-3、乌饭子3-4、间苯二甲酸-5-磺酸钠1-3、氯化钠10-12、槲皮素1-2、吐温80 1_2,其制备方法为:先将乌饭子放入10倍其重量份的水中,煎煮1-1.5h,过滤,所得滤液冷却至50-60°C时,加入氯化钠、吐温80、间苯二甲酸-5-磺酸钠,搅拌至混合物料完全溶解后,再加入其它剩余物料,继续搅拌溶解分散l_2h,即得助剂。

[0004] 所述的一种竹条改性用增韧保色浸泡液及其使用方法,其制备方法为:先将白果投入水中,煎煮2_3h,过滤,待所得滤液冷却至50_60°C后,加入硫酸锌、钼酸钠、尿素,搅拌至物料完全溶解后,再加入其它剩余物料,继续搅拌40-50min,即得浸泡液。

[0005] 所述的一种竹条改性用增韧保色浸泡液及其使用方法,其使用方法为:将预处理后的竹条完全没入上述浸泡液中,在50-60°C下保温密闭浸泡25-28h,取出清水洗净自然晾干或烘干即可。

[0006] 本发明的浸泡液优点在于:其采用的原料均为环保成分,不含挥发性毒性有机物成分,不污染使用环境,原料中的硫酸锌、钼酸钠、尿素、过氧碳酸钠等成分能够有效的软化竹条,改善塑性,达到促渗、阻燃、防腐、保色等功效,白果水煎液能驱虫防蛀,提高竹条对外界微生物的抵御能力;本发明浸泡液制备方法及使用方法简单,化学性能稳定,废液回收处理简单,改性后的竹条色泽明亮均匀,柔韧易塑,不易折断,生产效率获得提升,所得产品长时间不变色,不易霉腐虫蛀,阻燃安全,经久耐用。具体实施方式实施例

[0007] 本实施例的浸泡液由以下重量份(公斤)的原料制得:硫酸锌4、脂肪醇聚氧乙烯醚硫酸钠4、石油磺酸钠4、白果3、过氧碳酸钠8、钼酸钠6、尿素18、水280、助剂5 ;助剂由下列重量份的原料制成:二氢月桂烯醇2、乌饭子4、间苯二甲酸-5-磺酸钠3、氯化钠12、槲皮素1、吐温80 2,其制备方法为:先将乌饭子放入10倍其重量份的水中,煎煮1.5h,过滤,所得滤液冷却至50-60 0C时,加入氯化钠、吐温80、间苯二甲酸-5-磺酸钠,搅拌至混合物料完全溶解后,再加入其它剩余物料,继续搅拌溶解分散2h,即得助剂。

[0008] 本实施例的浸泡液制备方法为:先将白果投入水中,煎煮3h,过滤,待所得滤液冷却至50-60°C后,加入硫酸锌、钼酸钠、尿素,搅拌至物料完全溶解后,再加入其它剩余物料,继续搅拌50min,即得浸泡液。

[0009] 将预处理后的竹条完全没入上述浸泡液中,加热至50-60°C,保温密闭浸泡26h,取出清水洗净自然晾干或烘干,再进行后续工序。在后续编织过程中,本实施例浸泡液处理后的竹条抗冲击强度较传统方法处理的材料增加22.6%,弯曲强度提高27.5%,燃烧试验表明,改性后的竹条热释放速率降低58.6%,总放热率降低56.4%。处理后的材料编织时更容易,平均生产效率提高22.1%,产品放置2年以上无变色、腐蛀、裂纹等问题。

Claims (3)

1.一种竹条改性用增韧保色浸泡液及其使用方法,其特征在于,该浸泡液由以下重量份的原料制成:硫酸锌3-5、脂肪醇聚氧乙烯醚硫酸钠4-5、石油磺酸钠2-4、白果2-4、过氧碳酸钠6-9、钼酸钠5-8、尿素15-18、水250-280、助剂4-5 ; 助剂由下列重量份的原料制成:二氢月桂烯醇2-3、乌饭子3-4、间苯二甲酸-5-磺酸钠1-3、氯化钠10-12、槲皮素1-2、吐温80 1_2,其制备方法为:先将乌饭子放入10倍其重量份的水中,煎煮1-1.5h,过滤,所得滤液冷却至50-60°C时,加入氯化钠、吐温80、间苯二甲酸-5-磺酸钠,搅拌至混合物料完全溶解后,再加入其它剩余物料,继续搅拌溶解分散l_2h,即得助剂。
2.如权利要求1所述的一种竹条改性用增韧保色浸泡液及其使用方法,其制备方法为:先将白果投入水中,煎煮2-3h,过滤,待所得滤液冷却至50-60°C后,加入硫酸锌、钼酸钠、尿素,搅拌至物料完全溶解后,再加入其它剩余物料,继续搅拌40-50min,即得浸泡液。
3.如权利要求1所述的一种竹条改性用增韧保色浸泡液及其使用方法,其使用方法为:将预处理后的竹条完全没入上述浸泡液中,在50-60°C下保温密闭浸泡25-28h,取出清水洗净自然晾干或烘干即可。
CN201510365613.XA 2015-06-29 2015-06-29 一种竹条改性用增韧保色浸泡液及其使用方法 CN105128106A (zh)