CN105111857A - High-grade furniture transparent primer - Google Patents

High-grade furniture transparent primer Download PDF

Info

Publication number
CN105111857A
CN105111857A CN201510430025.XA CN201510430025A CN105111857A CN 105111857 A CN105111857 A CN 105111857A CN 201510430025 A CN201510430025 A CN 201510430025A CN 105111857 A CN105111857 A CN 105111857A
Authority
CN
China
Prior art keywords
speed mixer
copolymer resin
diatomite
ethylene glycol
titanium dioxide
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510430025.XA
Other languages
Chinese (zh)
Inventor
张友吉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
BIDEA FURNITURE GROUP CHINA Co Ltd
Original Assignee
BIDEA FURNITURE GROUP CHINA Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by BIDEA FURNITURE GROUP CHINA Co Ltd filed Critical BIDEA FURNITURE GROUP CHINA Co Ltd
Priority to CN201510430025.XA priority Critical patent/CN105111857A/en
Publication of CN105111857A publication Critical patent/CN105111857A/en
Pending legal-status Critical Current

Abstract

The invention discloses a high-grade furniture transparent primer, which is composed of the following raw materials by weight part: 22-25 of vinyl chloride copolymer resin, 3-5 of xylene, 8-10 of an elastic emulsion, 4-6 of ethylene glycol monobutyl ether, 1.5-2.5 of titanium dioxide, 1.4-1.8 of ethyl cellulose, 2.5-3.5 of diatomite, 2-4 of trimethylolpropane, 2.5-4.5 of cyclohexanone, 0.3-0.8 of a polyurethane thickening agent, 1.3-1.5 of an organic tin drier, 0.2-0.4 of a defoaming agent, and 23-25 of distilled water. By using the vinyl chloride copolymer resin, the paint viscosity can be strengthened, and crack does not appear when the paint is applied to furniture surface. The adopted raw materials are organic raw materials, are green, energy saving, safe and harmless to human, and therefore the paint has good gloss retention, high temperature resistance, water resistance and weather resistance.

Description

A kind of top-grade furniture transparent priming
Technical field
The present invention relates to decorative paint field, specifically belong to a kind of top-grade furniture transparent priming.
Background technology
Existing paint is on the market of a great variety, but along with people are to the increase of the functional requirement of paint, existing paint can not meet this needs of people, and paint has not been just realized protection, decoration functions just now.For the priming paint of top-grade furniture, raise variety seldom in market, and have the shortcomings such as expensive, environmental-protecting performance is poor, and various performance index are not good, and production process is complicated, and the function of paint need to enrich.
Summary of the invention
The object of this invention is to provide a kind of top-grade furniture transparent priming, use chloroethylene copolymer resin that paint viscosity can be made to strengthen and be coated in furniture surface, there will not be crackle, the raw material adopted mostly is organic raw material green, energy-conservation, safety is harmless to people, and the gloss retention thus painted, high thermal resistance, water tolerance and weathering resistance are better.
The technical solution used in the present invention is as follows:
A kind of top-grade furniture transparent priming, by weight, is made up of following raw material:
Chloroethylene copolymer resin 22-25, dimethylbenzene 3-5, elastic emulsion 8-10, ethylene glycol monobutyl ether 4-6, titanium dioxide 1.5-2.5, ethyl cellulose 1.4-1.8, diatomite 2.5-3.5, TriMethylolPropane(TMP) 2-4, pimelinketone 2.5-4.5, polyurethanes thickening material 0.3-0.8, organotin siccative 1.3-1.5, defoamer 0.2-0.4, distilled water 23-25;
Its concrete preparation method is as follows: add in high-speed mixer by chloroethylene copolymer resin, dimethylbenzene, diatomite and elastic emulsion, after high-speed mixing 50 ~ 80min, then in high-speed mixer, ethylene glycol monobutyl ether, titanium dioxide, defoamer and distilled water is added, cover tightly high-speed mixer, by the high-speed mixer that stops after above-mentioned material high-speed mixing 20 ~ 30min, the slip that high-speed mixer is released puts into colloidal mill circular grinding 35-40min, slurry after grinding fully mixes with surplus stock, low rate mixing 50-80min and get final product.
A kind of top-grade furniture transparent priming, is made up of following raw material: chloroethylene copolymer resin 23, dimethylbenzene 4, elastic emulsion 9, ethylene glycol monobutyl ether 5, titanium dioxide 2, ethyl cellulose 1.6, diatomite 3, TriMethylolPropane(TMP) 3, pimelinketone 3, polyurethanes thickening material 0.5, organotin siccative 1.4, defoamer 0.3, distilled water 24.
The present invention adopts elastic emulsion as emulsifying agent, use chloroethylene copolymer resin that paint viscosity can be made to strengthen and be coated in furniture surface, there will not be crackle, the raw material adopted mostly is organic raw material green, energy-conservation, safety is harmless to people, and the gloss retention thus painted, high thermal resistance, water tolerance and weathering resistance are better.
The test performance of the present invention's paint.
Air permeance resistance, Sd-value 0.032m is excellent
Sticking power 4.2N/mm 2excellent
Package stability, 28 days/50 DEG C excellent
Wet rubbing is washed, 4 days >2240 time.
Embodiment
A kind of top-grade furniture transparent priming, by weight, be made up of following raw material: chloroethylene copolymer resin 23, dimethylbenzene 4, elastic emulsion 9, ethylene glycol monobutyl ether 5, titanium dioxide 2, ethyl cellulose 1.6, diatomite 3, TriMethylolPropane(TMP) 3, pimelinketone 3, polyurethanes thickening material 0.5, organotin siccative 1.4, defoamer 0.3, distilled water 24;
Its concrete preparation method is as follows: add in high-speed mixer by chloroethylene copolymer resin, dimethylbenzene, diatomite and elastic emulsion, after high-speed mixing 65min, then in high-speed mixer, ethylene glycol monobutyl ether, titanium dioxide, defoamer and distilled water is added, cover tightly high-speed mixer, by the high-speed mixer that stops after above-mentioned material high-speed mixing 25min, the slip that high-speed mixer is released puts into colloidal mill circular grinding 38min, slurry after grinding fully mixes with surplus stock, low rate mixing 65min and get final product.

Claims (2)

1. a top-grade furniture transparent priming, by weight, is characterized in that, is made up of following raw material:
Chloroethylene copolymer resin 22-25, dimethylbenzene 3-5, elastic emulsion 8-10, ethylene glycol monobutyl ether 4-6, titanium dioxide 1.5-2.5, ethyl cellulose 1.4-1.8, diatomite 2.5-3.5, TriMethylolPropane(TMP) 2-4, pimelinketone 2.5-4.5, polyurethanes thickening material 0.3-0.8, organotin siccative 1.3-1.5, defoamer 0.2-0.4, distilled water 23-25;
Its concrete preparation method is as follows: add in high-speed mixer by chloroethylene copolymer resin, dimethylbenzene, diatomite and elastic emulsion, after high-speed mixing 50 ~ 80min, then in high-speed mixer, ethylene glycol monobutyl ether, titanium dioxide, defoamer and distilled water is added, cover tightly high-speed mixer, by the high-speed mixer that stops after above-mentioned material high-speed mixing 20 ~ 30min, the slip that high-speed mixer is released puts into colloidal mill circular grinding 35-40min, slurry after grinding fully mixes with surplus stock, low rate mixing 50-80min and get final product.
2. top-grade furniture transparent priming according to claim 1, it is characterized in that, be made up of following raw material: chloroethylene copolymer resin 23, dimethylbenzene 4, elastic emulsion 9, ethylene glycol monobutyl ether 5, titanium dioxide 2, ethyl cellulose 1.6, diatomite 3, TriMethylolPropane(TMP) 3, pimelinketone 3, polyurethanes thickening material 0.5, organotin siccative 1.4, defoamer 0.3, distilled water 24.
CN201510430025.XA 2015-07-20 2015-07-20 High-grade furniture transparent primer Pending CN105111857A (en)