CN104550676A - 聚乙烯醇脱模技术 - Google Patents

聚乙烯醇脱模技术 Download PDF

Info

Publication number
CN104550676A
CN104550676A CN201310538625.9A CN201310538625A CN104550676A CN 104550676 A CN104550676 A CN 104550676A CN 201310538625 A CN201310538625 A CN 201310538625A CN 104550676 A CN104550676 A CN 104550676A
Authority
CN
China
Prior art keywords
polyvinyl alcohol
technology
mass parts
ethanol
water
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310538625.9A
Other languages
English (en)
Inventor
刘继玲
Original Assignee
刘继玲
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 刘继玲 filed Critical 刘继玲
Priority to CN201310538625.9A priority Critical patent/CN104550676A/zh
Publication of CN104550676A publication Critical patent/CN104550676A/zh
Pending legal-status Critical Current

Abstract

一种聚乙烯醇溶液脱模剂制造新技术,该项技术所生产出的产品具有无毒、黏度小、最高使用温度达150度,若在120度下使用,脱模效果更好。本品主要用于手糊制品、成型形状复杂的大型制品,或与其他脱模剂复合使用。

Description

聚乙烯醇脱模技术
所属技术领域
:
[0001] 本发明涉及工业铸造用脱模剂利用技术领域,具体涉及一种利用聚乙烯醇溶液脱模新技术。
背景技术
:
[0002] 成型用的脱模剂是一种非常重要的原料,但由于生产方式不同,产品的质量也各有差异,制造成本也不一样,脱模效果差异很大,对环境的影响也不一样。
发明内容
[0003] 本发明提供了一种聚乙烯醇溶液脱模剂制造新技术。该项技术所生产出的产品具有无毒、黏度小、最高使用温度达150度,若在120度下使用,脱模效果更好。本品主要用于手糊制品、成型形状复杂的大型制品,或与其他脱模剂复合使用。
[0004] 这种聚乙烯醇溶液脱模剂的原料配方为:
[0005] 聚乙烯醇-(8-10)质量份,
[0006] 乙醇-(30-60)质量份,
[0007]水-(60-35)质量份。
[0008] 具体实施方法:
[0009] 将聚乙烯醇浸泡在装有水的容器中,常温放置3小时,然后逐渐升温至90度,待全部溶解后,冷却至60度,在搅拌下滴入乙醇,然后过滤得本产品。制造过程中,应注意以下几点;
[0010] (I)应用分子量较低和乙烯基含量在10% -35%的聚烯醇为好,这样溶解性好,可提高脱模效果,按需用确定水和乙醇比例,多加水可以使成膜均匀,多加乙醇可以使薄膜干燥速度加快。
[0011] (2)为了成膜均匀,可加入2%软皂。
[0012] (3)为了使涂膜性能良好,成膜平整、光滑,可加入少量气溶胶。
[0013] (4)为了消除气泡,可加入0.01%的硅油或磷酸三丁脂。
[0014] (5)为了使模具有韧性,可加入4%甘油作增塑剂。
[0015] (6)为了防止漏涂,可加入柏林蓝。
[0016] (7)为防止金属模具生锈,可加入1%的苯甲酸钠。

Claims (2)

1.一种聚乙烯醇溶液脱模新技术;其用料配方为,聚乙烯醇(8-10)质量份,乙醇(30-60)质量份,水(60-35)质量份。
2.其特征在于;所述的这种技术是按以下方法制备的,将聚乙烯醇浸泡在装有水的容器中,常温放置3小时,然后逐渐升温至90度,待全部溶解后,冷却至60度,在搅拌下滴入乙醇,然后过滤得本产品。
CN201310538625.9A 2013-10-27 2013-10-27 聚乙烯醇脱模技术 Pending CN104550676A (zh)