CN104475995B - 一种铲斗的焊接方法 - Google Patents
一种铲斗的焊接方法 Download PDFInfo
- Publication number
- CN104475995B CN104475995B CN201410615415.XA CN201410615415A CN104475995B CN 104475995 B CN104475995 B CN 104475995B CN 201410615415 A CN201410615415 A CN 201410615415A CN 104475995 B CN104475995 B CN 104475995B
- Authority
- CN
- China
- Prior art keywords
- scraper bowl
- welding
- bucket
- weld
- auxiliary frame
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本发明提供一种铲斗的焊接方法,所述铲斗包括连接面和工作面,连接面上设有限位块和加强筋;将铲斗平放在地面上,打底焊接的电流电压为正常焊接的0.9倍,焊接速度为正常焊接的1.2倍,打底焊缝从距刀板50‑100cm范围内开始;铲斗扣在辅助架顶上,铲斗扣在辅助架第二阶;本发明涉及的这种铲斗的焊接方法,使铲斗的焊接质量有所提高,延长铲斗的使用寿命。
Description
技术领域
本发明涉及一种铲斗的焊接方法,属于机械技术领域。
背景技术
现有的铲斗在焊接时,由于铲斗的摆放位置不够恰当,导致在施力焊接时的焊接质量不高,使铲斗在工作过程中,无法承担应有的重量,且其焊接处也容易发生断裂,导致焊接失败,以至于无法修复,使铲斗的使用寿命降低。
发明内容
本发明提供一种铲斗的焊接方法,使铲斗的焊接质量有所提高,延长铲斗的使用寿命。
为解决以上技术问题,本发明提供如下技术方案:一种铲斗的焊接方法,所述铲斗包括连接面和工作面,连接面上设有限位块和加强筋;将铲斗平放在地面上,打底焊接的电流电压为正常焊接的0.9倍,焊接速度为正常焊接的1.2倍,打底焊缝从距刀板50-100cm范围内开始;铲斗扣在辅助架顶上,铲斗扣在辅助架第二阶,使铲斗倾斜一定的角度;铲斗固定在变位机上将其竖起来摆到合适的角度,焊接方向为水平方向,从铲斗的弯曲方向沿至边沿;再竖直旋转180°,焊接铲斗工作面;再将铲斗水平方向旋转180°,调整合适焊接角度,焊接走向为从边沿至铲斗的曲面方向,水平焊接;再竖直旋转180度,焊接铲斗工作面;将铲斗水平放置,焊接连接面上的限位块和加强筋。
本发明涉及的这种铲斗的焊接方法,使铲斗的焊接质量有所提高,延长铲斗的使用寿命。
附图说明
图1为本发明铲斗平放时的结构图;
图2为本发明铲斗铺在辅助架上的结构图;
图3为本发明铲斗铺在辅助架第二阶的结构图;
图4为本发明铲斗竖直与变形位机固定后的结构图;
图5为本发明铲斗竖直旋转180°后的结构图;
图6为本发明铲斗水平旋转180°时的结构图;
图7为本发明铲斗竖直旋转180°时焊接内侧的结构图;
图8为本发明铲斗焊接限位块和加强筋时的结构图;
1-铲斗;2-辅助架。
具体实施方式
如图1-图8所示,一种铲斗的焊接方法,所述铲斗包括连接面和工作面,连接面上设有限位块和加强筋;将铲斗平放在地面上,打底焊接的电流电压为正常焊接的0.9倍,焊接速度为正常焊接的1.2倍,打底焊缝从距刀板50-100cm范围内开始;铲斗扣在辅助架顶上,铲斗扣在辅助架第二阶,使铲斗倾斜一定的角度;铲斗固定在变位机上将其竖起来摆到合适的角度,焊接方向为水平方向,从铲斗的弯曲方向沿至边沿;再竖直旋转180°,焊接铲斗工作面;再将铲斗水平方向旋转180°,调整合适焊接角度,焊接走向为从边沿至铲斗的曲面方向,水平焊接;再竖直旋转180度,焊接铲斗工作面;将铲斗水平放置,焊接连接面上的限位块和加强筋。
本发明涉及的这种铲斗的焊接方法,使铲斗的焊接质量有所提高,延长铲斗的使用寿命。
本发明所述的具体实施方式并不构成对本申请范围的限制,凡是在本发明构思的精神和原则之内,本领域的专业人员能够作出的任何修改、等同替换和改进等均应包含在本发明的保护范围之内。
Claims (1)
1.一种铲斗的焊接方法,所述铲斗包括连接面和工作面,连接面上设有限位块和加强筋,其特征在于,将铲斗平放在地面上,打底焊接的电流电压为正常焊接的0.9倍,焊接速度为正常焊接的1.2倍,打底焊缝从距刀板50-100cm范围内开始;铲斗扣在辅助架顶上,铲斗扣在辅助架第二阶,使铲斗倾斜一定的角度;铲斗固定在变位机上将其竖起来摆到合适的角度,焊接方向为水平方向,从铲斗的弯曲方向沿至边沿;再竖直旋转180°,焊接铲斗工作面;再将铲斗水平方向旋转180°,调整合适焊接角度,焊接走向为从边沿至铲斗的曲面方向,水平焊接;再竖直旋转180度,焊接铲斗工作面;将铲斗水平放置,焊接连接面上的限位块和加强筋。