CN104371482A - 一种耐高温机械涂料 - Google Patents

一种耐高温机械涂料 Download PDF

Info

Publication number
CN104371482A
CN104371482A CN201410600861.3A CN201410600861A CN104371482A CN 104371482 A CN104371482 A CN 104371482A CN 201410600861 A CN201410600861 A CN 201410600861A CN 104371482 A CN104371482 A CN 104371482A
Authority
CN
China
Prior art keywords
parts
temperature resistant
mechanical coating
resistant mechanical
coating
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410600861.3A
Other languages
English (en)
Inventor
杨龙兴
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Wuxi Yanggong Machinery Manufacturing Co Ltd
Original Assignee
Wuxi Yanggong Machinery Manufacturing Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Wuxi Yanggong Machinery Manufacturing Co Ltd filed Critical Wuxi Yanggong Machinery Manufacturing Co Ltd
Priority to CN201410600861.3A priority Critical patent/CN104371482A/zh
Publication of CN104371482A publication Critical patent/CN104371482A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种耐高温机械涂料,各组分按重量份计:丁醚化脲醛树脂100份、环氧树脂36-41份、偏氯乙烯12-19份、醇酸聚氨酯3-10份、松油1-5份。本发明提供的耐高温机械涂料,在长时间的日晒下或高温环境下,仍具有很好的粘结性,保证了机械部件高温条件下作业的安全。

Description

一种耐高温机械涂料
技术领域
本发明涉及一种涂料。
背景技术
机械涂料就是指涂装在机械表面及各类机器零部件上的涂料。机械涂料具有以下性能:
(1)遮盖力:
遮盖力通常用能使规定的黑白格掩盖所需的涂料重量来表示,重量越大遮盖力越小。
(2)涂抹附着力:
表示涂膜与基层的粘合力。
(3)粘度:
粘度的大小影响施工性能,不同的施工方法要求涂料有不同的粘度。
(4)细度:
细度大小直接影响涂膜表面的平整性和光泽。
现有的机械涂料,主要作用是降防止机械部件与外界隔离开来,避免机械部件被氧化、腐蚀。但是,现有的机械涂料的耐高温性能还不够,在高温和长期日晒的环境下,很容易脱落。
发明内容
本发明要解决的技术问题是克服现有的缺陷,提供了一种耐高温机械涂料。
本发明的目的通过以下技术方案来具体实现:
一种耐高温机械涂料,各组分按重量份计:丁醚化脲醛树脂100份、环氧树脂36-41份、偏氯乙烯12-19份、醇酸聚氨酯3-10份、松油1-5份。
作为优选方案,上述的耐高温机械涂料,各组分按重量份计:丁醚化脲醛树脂100份、环氧树脂37份、偏氯乙烯15份、醇酸聚氨酯5.5份、松油5份。
本发明的有益效果:
本发明提供的耐高温机械涂料,在长时间的日晒下或高温环境下,仍具有很好的粘结性,保证了机械部件高温条件下作业的安全。
具体实施方式
以下对本发明的优选实施例进行说明,应当理解,此处所描述的优选实施例仅用于说明和解释本发明,并不用于限定本发明。
实施例1:
一种耐高温机械涂料,各组分按重量份计:丁醚化脲醛树脂100份、环氧树脂37份、偏氯乙烯15份、醇酸聚氨酯5.5份、松油5份。
实施例2:
一种耐高温机械涂料,各组分按重量份计:丁醚化脲醛树脂100份、环氧树脂36份、偏氯乙烯19份、醇酸聚氨酯3份、松油5份。
实施例3:
一种耐高温机械涂料,各组分按重量份计:丁醚化脲醛树脂100份、环氧树脂41份、偏氯乙烯12份、醇酸聚氨酯10份、松油1份。
以上所述仅为本发明的优选实施例而已,并不用于限制本发明,尽管参照前述实施例对本发明进行了详细的说明,对于本领域的技术人员来说,其依然可以对前述各实施例所记载的技术方案进行修改,或者对其中部分技术特征进行等同替换。凡在本发明的精神和原则之内,所作的任何修改、等同替换、改进等,均应包含在本发明的保护范围之内。

Claims (2)

1.一种耐高温机械涂料,其特征在于:各组分按重量份计:丁醚化脲醛树脂100份、环氧树脂36-41份、偏氯乙烯12-19份、醇酸聚氨酯3-10份、松油1-5份。
2.根据权利要求1所述的耐高温机械涂料,其特征在于:各组分按重量份计:丁醚化脲醛树脂100份、环氧树脂37份、偏氯乙烯15份、醇酸聚氨酯5.5份、松油5份。
CN201410600861.3A 2014-10-31 2014-10-31 一种耐高温机械涂料 Pending CN104371482A (zh)