CN104308367A CN201410588577.9A CN201410588577A CN104308367A CN 104308367 A CN104308367 A CN 104308367A CN 201410588577 A CN201410588577 A CN 201410588577A CN 104308367 A CN104308367 A CN 104308367A
Authority
CN
China
Prior art keywords
welded
welded plate
stainless steel
lower plate
upper plate
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410588577.9A
Other languages
English (en)
Inventor
何晓阳
朱文琪
陈晓磊
张乾
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
WUXI HANSHEN ELECTRIC CO Ltd
Original Assignee
WUXI HANSHEN ELECTRIC CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by WUXI HANSHEN ELECTRIC CO Ltd filed Critical WUXI HANSHEN ELECTRIC CO Ltd
Priority to CN201410588577.9A priority Critical patent/CN104308367A/zh
Publication of CN104308367A publication Critical patent/CN104308367A/zh
Pending legal-status Critical Current

Links

Abstract

本发明涉及一种不锈钢激光叠焊装置,它包括待焊上板、待焊下板、冷却衬垫、夹具与激光焊接头;在冷却衬垫的上表面放置有待焊下板,在待焊下板的上表面放置有待焊上板,待焊上板与待焊下板呈面接触,所述夹具将在待焊上板、待焊下板与冷却衬垫夹紧,在待焊上板的上方设有激光焊接头。本发明通过在焊缝背面加冷却衬垫,并采用夹具将待焊上板、待焊下板与冷却衬垫压紧后进行焊接,即可得到焊缝背面无明显焊接痕迹且焊缝性能满足要求的叠焊焊缝。

Description

不锈钢激光叠焊装置
技术领域
[0001] 本发明涉及一种激光焊接装置,本发明尤其是涉及一种不锈钢激光叠焊装置。
背景技术
[0002] 在已有技术中,不锈钢叠焊大多采用电阻焊进行焊接,其很容易在焊接处留下焊接压痕,严重影响成品外观,不能满足一些对外观要求较高的产品。激光焊接由于其热输入量小,焊接变形小,在焊接领域具有很大的优势。但采用传统的激光焊接工艺进行不锈钢叠焊仍能在不锈钢表面留下很明显的焊接痕迹。
发明内容
[0003] 本发明的目的是克服现有技术中存在的不足,提供一种可大幅减小焊缝背面不锈钢表面的焊接痕迹、提闻焊接质量的不镑钢激光置焊装置。
[0004] 按照本发明提供的技术方案,所述不锈钢激光叠焊装置,它包括待焊上板、待焊下板、冷却衬垫、夹具与激光焊接头;在冷却衬垫的上表面放置有待焊下板,在待焊下板的上表面放置有待焊上板,待焊上板与待焊下板呈面接触,所述夹具将在待焊上板、待焊下板与冷却衬垫夹紧,在待焊上板的上方设有激光焊接头。
[0005] 所述待焊上板的厚度小于待焊下板的厚度。
[0006] 所述待焊上板的厚度为0.6^1.0mm。
[0007] 所述待焊下板的厚度为1.5^2.5mm。
[0008] 本发明通过在焊缝背面加冷却衬垫,并采用夹具将待焊上板、待焊下板与冷却衬垫压紧后进行焊接,即可得到焊缝背面无明显焊接痕迹且焊缝性能满足要求的叠焊焊缝。
附图说明
[0009] 图1是本发明的结构示意图。
具体实施方式
[0010] 下面结合具体实施例对本发明作进一步说明。
[0011] 该不锈钢激光叠焊装置,它包括待焊上板1、待焊下板2、冷却衬垫3、夹具4与激光焊接头5 ;在冷却衬垫3的上表面放置有待焊下板2,在待焊下板2的上表面放置有待焊上板1,待焊上板I与待焊下板2呈面接触,所述夹具4将在待焊上板1、待焊下板2与冷却衬垫3夹紧,在待焊上板I的上方设有激光焊接头5。
[0012] 所述待焊上板I的厚度小于待焊下板2的厚度。
[0013] 所述待焊上板I的厚度为0.6〜1.0mm。
[0014] 所述待焊下板2的厚度为1.5^2.5mm。
[0015] 工作时,先清理待焊上板I与待焊下板2对接面,用酒精擦洗对接面,叠放在冷却衬垫3上,用夹具4压紧。
[0016] 调整激光焊接头5的焊接工艺参数:功率为1400W、离焦量为O、焊接速度为3000mm/min、保护气体流量为15L/min。
[0017] 离焦量为O时,激光光斑最小,便可在较低热输入下实现较大熔深。另外由于冷却衬垫3和夹具4的作用使得焊接变形进一步减小。通过此装置便可使焊缝背面几乎没有焊接痕迹。

Claims (4)

1.一种不锈钢激光叠焊装置,其特征是:它包括待焊上板(I)、待焊下板(2)、冷却衬垫(3)、夹具(4)与激光焊接头(5);在冷却衬垫(3)的上表面放置有待焊下板(2),在待焊下板(2 )的上表面放置有待焊上板(I),待焊上板(I)与待焊下板(2 )呈面接触,所述夹具(4 )将在待焊上板(I)、待焊下板(2)与冷却衬垫(3)夹紧,在待焊上板(I)的上方设有激光焊接头(5)。
2.如权利要求1所述的不锈钢激光叠焊装置,其特征是:所述待焊上板(I)的厚度小于待焊下板(2)的厚度。
3.如权利要求1所述的不锈钢激光叠焊装置,其特征是:所述待焊上板(I)的厚度为.0.6〜1.0mm。
4.如权利要求1所述的不锈钢激光叠焊装置,其特征是:所述待焊下板(2)的厚度为.1.5〜2.5mm。
CN201410588577.9A 2014-10-28 2014-10-28 不锈钢激光叠焊装置 Pending CN104308367A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201410588577.9A CN104308367A (zh) 2014-10-28 2014-10-28 不锈钢激光叠焊装置

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201410588577.9A CN104308367A (zh) 2014-10-28 2014-10-28 不锈钢激光叠焊装置

Publications (1)

Publication Number Publication Date
CN104308367A true CN104308367A (zh) 2015-01-28

Family

ID=52363752

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201410588577.9A Pending CN104308367A (zh) 2014-10-28 2014-10-28 不锈钢激光叠焊装置

Country Status (1)

Country Link
CN (1) CN104308367A (zh)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN105728492A (zh) * 2016-03-11 2016-07-06 华中科技大学 一种屈服强度大于700MPa的复合钢板及其制备方法
CN112207442A (zh) * 2020-10-14 2021-01-12 华中科技大学 抑制厚板激光穿透焊接下塌缺陷的方法及气体加载装置

Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2001252777A (ja) * 2000-03-09 2001-09-18 Laser Oyo Kogaku Kenkyusho:Kk 異種金属のレーザー接合方法
CN201645047U (zh) * 2010-02-09 2010-11-24 重庆远雄制冷成套设备有限公司 薄板叠焊用焊接设备
CN102240852A (zh) * 2011-05-20 2011-11-16 无锡汉神电气有限公司 镀锌板激光叠焊装置
CN102922817A (zh) * 2012-11-20 2013-02-13 无锡汉神电气有限公司 用于激光叠焊的镀锌板及其焊接工艺
EP2777864A1 (de) * 2013-03-14 2014-09-17 BSH Bosch und Siemens Hausgeräte GmbH Verfahren zum Verbinden von zwei Blechplatten eines Haushaltsgeräts mit überlappenden Laserschweissen von unterschiedlichen Edelstählen; entsprechendes Haushaltsgerät

Patent Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2001252777A (ja) * 2000-03-09 2001-09-18 Laser Oyo Kogaku Kenkyusho:Kk 異種金属のレーザー接合方法
CN201645047U (zh) * 2010-02-09 2010-11-24 重庆远雄制冷成套设备有限公司 薄板叠焊用焊接设备
CN102240852A (zh) * 2011-05-20 2011-11-16 无锡汉神电气有限公司 镀锌板激光叠焊装置
CN102922817A (zh) * 2012-11-20 2013-02-13 无锡汉神电气有限公司 用于激光叠焊的镀锌板及其焊接工艺
EP2777864A1 (de) * 2013-03-14 2014-09-17 BSH Bosch und Siemens Hausgeräte GmbH Verfahren zum Verbinden von zwei Blechplatten eines Haushaltsgeräts mit überlappenden Laserschweissen von unterschiedlichen Edelstählen; entsprechendes Haushaltsgerät

Non-Patent Citations (1)

* Cited by examiner, † Cited by third party
Title
刘佳: "轨道客车用SUS301L奥氏体不锈钢激光叠焊技术研究", 《中国博士学位论文全文数据库工程科技I辑》, 15 January 2013 (2013-01-15) *

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN105728492A (zh) * 2016-03-11 2016-07-06 华中科技大学 一种屈服强度大于700MPa的复合钢板及其制备方法
CN112207442A (zh) * 2020-10-14 2021-01-12 华中科技大学 抑制厚板激光穿透焊接下塌缺陷的方法及气体加载装置

Similar Documents

Publication Publication Date Title
CN104308367A (zh) 不锈钢激光叠焊装置
CN204545707U (zh) 不锈钢激光叠焊装置
CN203031117U (zh) 一种点焊机焊头结构
CN102744344B (zh) 刀背成形机
CN204657635U (zh) 新型基于plc控制装置的锯床
CN202212689U (zh) 铜带软连接件扩散焊接系统
CN203635678U (zh) 保护器钢套焊口压平装置
CN203343649U (zh) 锂电池激光焊接机的压合机构
CN205414721U (zh) 压力传感器激光焊接夹具
CN204584527U (zh) 一种门式埋弧焊机
CN203945015U (zh) 一种全铝水箱连接柱焊接定位工作台
CN205096374U (zh) 一种消声器上、下壳体接合冲压模具
CN204339132U (zh) 杯体激光焊接用夹具
CN205128705U (zh) 一种汽车消音器外壳拉伸装置
CN204545706U (zh) 能防止焊缝下凹的激光焊焊接装置
CN104057217B (zh) 一种芳香助焊剂
CN203265919U (zh) 激光拼焊工作台
CN204075441U (zh) 一种先导串焊机施压装置
CN203484774U (zh) 一种侧焊/感应钎焊触头组件用缓压式压头
CN203992802U (zh) 焊接铜环
CN204700458U (zh) 点焊接机构
CN205230802U (zh) 一种大型变压器器身压装结构
CN205414043U (zh) 一种铜壶壶盖的成型装置
CN203992804U (zh) 一种快速装夹焊极装置
CN205237390U (zh) 电流互感器一次导杆焊接工装

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C12 Rejection of a patent application after its publication
RJ01 Rejection of invention patent application after publication

Application publication date: 20150128