CN104057012A - 一种可塑性好型砂及其制备方法 - Google Patents

一种可塑性好型砂及其制备方法 Download PDF

Info

Publication number
CN104057012A
CN104057012A CN201410229221.6A CN201410229221A CN104057012A CN 104057012 A CN104057012 A CN 104057012A CN 201410229221 A CN201410229221 A CN 201410229221A CN 104057012 A CN104057012 A CN 104057012A
Authority
CN
China
Prior art keywords
parts
molding sand
plasticity
sand
kyanite
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410229221.6A
Other languages
English (en)
Inventor
朱安会
马洪章
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Anhui Xin Run Type Material Co Ltd
Original Assignee
Anhui Xin Run Type Material Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Anhui Xin Run Type Material Co Ltd filed Critical Anhui Xin Run Type Material Co Ltd
Priority to CN201410229221.6A priority Critical patent/CN104057012A/zh
Publication of CN104057012A publication Critical patent/CN104057012A/zh
Pending legal-status Critical Current

Abstract

一种可塑性好型砂,由下列重量份的原料制成:石英砂200-240、绢云母30-35、蓝晶石60-70、碳酸钙15-20、粘土10-15、木糖醇3-4、玉米芯30-40、聚四氟乙烯4-6、夕线石20-30、氧化锆2-4、氢氧化钠1-2、橄榄油脂肪酸3-4、蓖麻油3-4、松香酸钠4-5、水适量。本发明使用了蓝晶石、绢云母,经煅烧,结合加木糖醇、聚四氟乙烯、蓖麻油等粘结剂,使得型砂具有湿粘结性好、可塑性好,高温溃散性好,耐高温,制得的铸件尺寸精确,表面缩孔、缩松现象少,且无环境污染,具有很好的经济价值。

Description

技术领域
[0001] 本发明涉及铸造领域,尤其涉及一种可塑性好型砂及其制备方法。 一种可塑性好型砂及其制备方法
背景技术
[0002] 型砂是在铸造中用来造型的材料。型砂一般由铸造用原砂、型砂粘结剂和辅加物 等造型材料按一定的比例混合而成,也可用天然含粘土的硅砂,通常的铸铝用的型砂配方 中型砂粒径太大或太小,型砂料径太大,虽然透气性较好,但是铝砂件表面比较粗糙,光洁 度不好,型砂料径太小,导致砂型透气性不好,铝铸件有气孔产生。国内外广泛使用的煤粉 粘土湿型砂,一般由原砂、粘结剂、煤粉添加物等与水混制而成,具有一定的防粘砂效果和 材料成本低、生产效率高的优点,但其消耗量大、排放严重、在铸造过程煤粉燃烧分解产生 有毒气体污染。
[0003] 型砂按所用粘结剂不同,可分为粘土砂、水玻璃砂、水泥砂、石英砂等,以粘土砂、 水玻璃砂及石英砂用的最多。型砂在铸造生产中的作用极为重要,因型砂的质量不好而造 成的铸件废品约占铸件总废品的30〜50%。通常对型砂的要求是:1、具有较高的强度和热 稳定性,以承受各种外力和高温的作用。2、良好的流动性,即型砂在外力或本身重力作用下 砂粒间相互移动的能力。3、一定的可塑性,即型砂在外力作用下变形,当外力去除后能保持 所给予的形状的能力。4、较好的透气性,即型砂孔隙透过气体的能力。5、高的溃散性,又称 出砂性,即在铸件凝固后型砂是否容易破坏,是否容易从铸件上清除的性能。
[0004] 目前的铸造领域发展迅速,对于铸钢件和铸铁件的性能要求更高,从而要求进一 步提升型砂的性能。
发明内容
[0005] 本发明的目的在于提供一种可塑性好型砂及其制备方法,该型砂具有高的耐热 性、可塑性好、透气性好、粘结性好的特点。
[0006] 本发明的技术方案如下: 一种可塑性好型砂,其特征在于由下列重量份的原料制成:石英砂200-240、絹云母 30-35、蓝晶石60-70、碳酸钙15-20、粘土 10-15、木糖醇3-4、玉米芯30-40、聚四氟乙烯 4-6、夕线石20-30、氧化锆2-4、氢氧化钠1-2、橄榄油脂肪酸3-4、蓖麻油3-4、松香酸钠 4-5、水适量。
[0007] 所述可塑性好型砂的制备方法,其特征在于包括以下步骤:将石英砂、絹云母、 蓝晶石、碳酸钙、玉米芯、夕线石、粘土放入510-530°c煅烧炉中煅烧3-4小时,然后取 出,粉碎成200-300目粉末,然后加入氢氧化钠、松香酸钠、适量水,搅拌分散,练泥,送入 1410-1440°C煅烧炉中煅烧3-5小时,取出粉碎至50-100目,得到煅烧料;将氧化锆、木糖 醇、聚四氟乙烯、橄榄油脂肪酸混合,研磨30-40分钟,与煅烧料、其它剩余成分混合15-20 分钟,即得。
[0008] 本发明的有益效果

Claims (2)

1. 一种可塑性好型砂,其特征在于由下列重量份的原料制成:石英砂200-240、絹云 母30-35、蓝晶石60-70、碳酸钙15-20、粘土 10-15、木糖醇3-4、玉米芯30-40、聚四氟乙 烯4-6、夕线石20-30、氧化锆2-4、氢氧化钠1-2、橄榄油脂肪酸3-4、蓖麻油3-4、松香酸钠 4-5、水适量。
2. 根据权利要求1所述可塑性好型砂的制备方法,其特征在于包括以下步骤:将石英 砂、絹云母、蓝晶石、碳酸钙、玉米芯、夕线石、粘土放入510-530°C煅烧炉中煅烧3-4小时, 然后取出,粉碎成200-300目粉末,然后加入氢氧化钠、松香酸钠、适量水,搅拌分散,练泥, 送入1410-1440°C煅烧炉中煅烧3-5小时,取出粉碎至50-100目,得到煅烧料;将氧化锆、 木糖醇、聚四氟乙烯、橄榄油脂肪酸混合,研磨30-40分钟,与煅烧料、其它剩余成分混合 15-20分钟,即得。
CN201410229221.6A 2014-05-28 2014-05-28 一种可塑性好型砂及其制备方法 Pending CN104057012A (zh)