CN103643492B - 织物用柔软整理剂的制备方法 - Google Patents

织物用柔软整理剂的制备方法 Download PDF

Info

Publication number
CN103643492B
CN103643492B CN201310625478.9A CN201310625478A CN103643492B CN 103643492 B CN103643492 B CN 103643492B CN 201310625478 A CN201310625478 A CN 201310625478A CN 103643492 B CN103643492 B CN 103643492B
Authority
CN
China
Prior art keywords
parts
mass
solution
finishing agent
fatty
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310625478.9A
Other languages
English (en)
Other versions
CN103643492A (zh
Inventor
王开发
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
CHANGSHU XIONGFA KNITTING PLUSH Co Ltd
Original Assignee
CHANGSHU XIONGFA KNITTING PLUSH Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by CHANGSHU XIONGFA KNITTING PLUSH Co Ltd filed Critical CHANGSHU XIONGFA KNITTING PLUSH Co Ltd
Priority to CN201310625478.9A priority Critical patent/CN103643492B/zh
Publication of CN103643492A publication Critical patent/CN103643492A/zh
Application granted granted Critical
Publication of CN103643492B publication Critical patent/CN103643492B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种织物用柔软整理剂的制备方法,包括如下步骤:1)将脂肪醇聚氧乙烯醚、聚醚、三乙醇胺、蓖麻油、丙二醇混合,搅拌均匀,得溶液A;2)将十二烷基三甲基氯化铵、脂肪醇磷酸酯、月桂酰氨乙基硫酸钠、脂肪醇聚乙二醇酯、季戊四醇脂肪酸酯溶于水中,搅拌混合均匀,得溶液B;3)将溶液A和溶液B混合,升温至63~65℃,反应4~5小时;4)冷却至室温,加入1~2质量份羟丙基甲基纤维素、2~3质量份羟乙基脂肪酰胺、2~3质量份十八胺、200~250质量份水、7~9质量份脂肪醇聚乙二醇酯,搅拌混合均匀,即得成品。本发明制备的织物用柔软整理剂使织物具有良好的耐洗涤性,能获得持久的柔软效果。

Description

织物用柔软整理剂的制备方法
技术领域
本发明涉及织物用柔软整理剂的制备方法。
背景技术
目前常用的织物用柔软整理剂,不具有良好的耐洗涤性,织物的柔软效果不持久。
发明内容
本发明的目的在于提供一种织物用柔软整理剂的制备方法,其制备的织物用柔软整理剂使织物具有良好的耐洗涤性,能获得持久的柔软效果。
为实现上述目的,本发明的技术方案是设计一种织物用柔软整理剂的制备方法,包括如下步骤:
1)将1~2质量份脂肪醇聚氧乙烯醚、8~9质量份聚醚、2~3质量份三乙醇胺、5~8质量份蓖麻油、25~30质量份丙二醇混合,搅拌均匀,得溶液A;
2)将2~3质量份十二烷基三甲基氯化铵、15~18质量份脂肪醇磷酸酯、1~2质量份月桂酰氨乙基硫酸钠、1~2质量份脂肪醇聚乙二醇酯、6~8质量份季戊四醇脂肪酸酯溶于水中,搅拌混合均匀,得溶液B;
3)将溶液A和溶液B混合,升温至63~65℃,反应4~5小时;
4)冷却至室温,加入1~2质量份羟丙基甲基纤维素、2~3质量份羟乙基脂肪酰胺、2~3质量份十八胺、200~250质量份水、7~9质量份脂肪醇聚乙二醇酯,搅拌混合均匀,即得成品。
本发明的优点和有益效果在于:提供一种织物用柔软整理剂的制备方法,其制备的织物用柔软整理剂使织物具有良好的耐洗涤性,能获得持久的柔软效果。
具体实施方式
下面结合实施例,对本发明的具体实施方式作进一步描述。以下实施例仅用于更加清楚地说明本发明的技术方案,而不能以此来限制本发明的保护范围。
本发明具体实施的技术方案是:
实施例1
一种织物用柔软整理剂的制备方法,包括如下步骤:
1)将2质量份脂肪醇聚氧乙烯醚、9质量份聚醚、3质量份三乙醇胺、8质量份蓖麻油、30质量份丙二醇混合,搅拌均匀,得溶液A;
2)将3质量份十二烷基三甲基氯化铵、18质量份脂肪醇磷酸酯、2质量份月桂酰氨乙基硫酸钠、2质量份脂肪醇聚乙二醇酯、8质量份季戊四醇脂肪酸酯溶于水中,搅拌混合均匀,得溶液B;
3)将溶液A和溶液B混合,升温至65℃,反应5小时;
4)冷却至室温,加入2质量份羟丙基甲基纤维素、3质量份羟乙基脂肪酰胺、3质量份十八胺、250质量份水、9质量份脂肪醇聚乙二醇酯,搅拌混合均匀,即得成品。
实施例2
一种织物用柔软整理剂的制备方法,包括如下步骤:
1)将1质量份脂肪醇聚氧乙烯醚、8质量份聚醚、2质量份三乙醇胺、5质量份蓖麻油、25质量份丙二醇混合,搅拌均匀,得溶液A;
2)将2质量份十二烷基三甲基氯化铵、15质量份脂肪醇磷酸酯、1质量份月桂酰氨乙基硫酸钠、1质量份脂肪醇聚乙二醇酯、6质量份季戊四醇脂肪酸酯溶于水中,搅拌混合均匀,得溶液B;
3)将溶液A和溶液B混合,升温至63℃,反应4小时;
4)冷却至室温,加入1质量份羟丙基甲基纤维素、2质量份羟乙基脂肪酰胺、2质量份十八胺、200质量份水、7质量份脂肪醇聚乙二醇酯,搅拌混合均匀,即得成品。
实施例3
一种织物用柔软整理剂的制备方法,包括如下步骤:
1)将1.2质量份脂肪醇聚氧乙烯醚、8.9质量份聚醚、2.3质量份三乙醇胺、5.8质量份蓖麻油、27质量份丙二醇混合,搅拌均匀,得溶液A;
2)将2.3质量份十二烷基三甲基氯化铵、16质量份脂肪醇磷酸酯、1.2质量份月桂酰氨乙基硫酸钠、1.2质量份脂肪醇聚乙二醇酯、6.8质量份季戊四醇脂肪酸酯溶于水中,搅拌混合均匀,得溶液B;
3)将溶液A和溶液B混合,升温至64℃,反应4.5小时;
4)冷却至室温,加入1.2质量份羟丙基甲基纤维素、2.3质量份羟乙基脂肪酰胺、2.3质量份十八胺、230质量份水、7.9质量份脂肪醇聚乙二醇酯,搅拌混合均匀,即得成品。
以上所述仅是本发明的优选实施方式,应当指出,对于本技术领域的普通技术人员来说,在不脱离本发明技术原理的前提下,还可以做出若干改进和润饰,这些改进和润饰也应视为本发明的保护范围。

Claims (1)

1.织物用柔软整理剂的制备方法,其特征在于,包括如下步骤:
1)将1~2质量份脂肪醇聚氧乙烯醚、8~9质量份聚醚、2~3质量份三乙醇胺、5~8质量份蓖麻油、25~30质量份丙二醇混合,搅拌均匀,得溶液A;
2)将2~3质量份十二烷基三甲基氯化铵、15~18质量份脂肪醇磷酸酯、1~2质量份月桂酰氨乙基硫酸钠、1~2质量份脂肪醇聚乙二醇酯、6~8质量份季戊四醇脂肪酸酯溶于水中,搅拌混合均匀,得溶液B;
3)将溶液A和溶液B混合,升温至63~65℃,反应4~5小时;
4)冷却至室温,加入1~2质量份羟丙基甲基纤维素、2~3质量份羟乙基脂肪酰胺、2~3质量份十八胺、200~250质量份水、7~9质量份脂肪醇聚乙二醇酯,搅拌混合均匀,即得成品。
CN201310625478.9A 2013-12-02 2013-12-02 织物用柔软整理剂的制备方法 Active CN103643492B (zh)