CN103512545B - 一种混凝土大坝内部裂缝监测方法及监测仪 - Google Patents
一种混凝土大坝内部裂缝监测方法及监测仪 Download PDFInfo
- Publication number
- CN103512545B CN103512545B CN201310453761.8A CN201310453761A CN103512545B CN 103512545 B CN103512545 B CN 103512545B CN 201310453761 A CN201310453761 A CN 201310453761A CN 103512545 B CN103512545 B CN 103512545B
- Authority
- CN
- China
- Prior art keywords
- range
- precision
- monitor
- sensor
- sensors
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
本发明是一种混凝土大坝内部裂缝监测方法及监测仪。方法是在混凝土坝钻孔内平行布置2条量程和精度均不同的监测仪。解决了混凝土大坝内部裂缝难以跟踪监测、监测范围有限、仪器精度不够的问题。监测仪构成为:由多个传感器经加长杆串联而成,传感器分别为小量程高精度传感器和大量程传感器。以满足混凝土坝体内部裂缝不同发展阶段的监测要求。当裂缝出现在仪器布置范围内时,即可测得裂缝变形值。
Description
技术领域
本发明涉及水电工程技术领域,具体说是一种混凝土大坝内部裂缝监测方法及监测仪。
背景技术
裂缝是混凝土大坝最常见的病害之一,列各类病害前列。我国是世界坝工大国,修建了8万多座坝,其中15m以上的大坝约1.8万余座,居世界第一。近年大坝建设发展尤其迅速,以三峡大坝(坝高181m)、金沙江溪洛渡拱坝(坝高285.5m)等为代表的一批的高坝大库日益增多,大坝的裂缝问题也越来越引起人们的重视。特别是随着三峡等大坝裂缝的出现,大坝混凝土内部裂缝的有效监测,已成为需要迫切解决的技术问题。
传统的裂缝监测仪器主要是测缝计、裂缝计等,主要用于物体表面已有裂缝监测,对于混凝土大坝坝体内部细微裂缝跟踪监测无能为力,因此急需需求一种满足混凝土大坝内部裂缝监测的技术和仪器。
发明内容
本发明的目的是提供一种混凝土大坝内部裂缝监测方法及监测仪,以解决目前混凝土大坝内部出现裂缝难以跟踪监测、监测范围有限、仪器精度不够的问题。
本发明的技术方案为:在混凝土坝钻孔内平行布置2条量程和精度均不同的监测仪。当裂缝出现在仪器布置范围内时,即可测得裂缝变形值。
所述的监测仪构成为:由多个传感器经加长杆串联而成,传感器分别为小量程高精度传感器和大量程传感器,以满足混凝土坝体内部裂缝不同发展阶段的监测要求。
传感器外包裹包柔性泡沫管与混凝土隔离,加长杆外包PVC材质的保护管以防止水泥浆粘结影响测量结果。
本发明的混凝土大坝内部裂缝监测仪器解决了混凝土大坝内部裂缝难以跟踪监测、监测范围有限、仪器精度不够的问题。当裂缝出现在仪器布置范围内时,即可测得裂缝变形值。本发明已成功应用于水电工程,取得了良好的效果,实用性强。本发明改变了我国混凝土大坝内部裂缝的监测方式,在混凝土坝中具有广泛的市场前景和推广价值。
附图说明
图1为本发明的混凝土坝内部裂缝监测仪器布置示意图。
图2为本发明的混凝土大坝内部裂缝监测仪器结构示意图。
图中:1-电缆,2-大量程传感器,3-小量程高精度传感器,4-加长杆,5-泡沫管,6-保护管,7-法兰盘。
具体实施方式
如图1所示,本发明的混凝土大坝内部裂缝监测方法是在混凝土坝钻孔内平行布置2条量程和精度均不同的监测仪。
所述的监测仪构成为:由多个传感器经金属加长杆4串联而成,加长后仪器标距均为1m,以满足沿钻孔的连续裂缝监测要求。传感器分别为小量程高精度传感器3(最大量程0.5mm、精度0.001mm)和大量程传感器2(最大量程5mm、精度0.01mm),以满足混凝土坝体内部裂缝不同发展阶段的监测要求。小量程高精度的裂缝监测仪器满足裂缝发展初期细微裂缝监测要求,解决了传统裂缝监测仪器精度不够的问题;大量程传感器满足裂缝发展后期或超过0.5mm宽度裂缝的监测要求。
传感器外包裹包柔性泡沫管5与混凝土隔离,金属加长杆外包PVC材质的保护管6以防止水泥浆粘结影响测量结果。仪器安装埋设后,通过灌浆管回填水泥浆,达到龄期后即可进行裂缝监测。每支传感器电缆1集中后熔接成多芯电缆引出,以避免电缆过多影响灌浆效果。
Claims (2)
1.一种混凝土大坝内部裂缝监测方法,其特征在于,在混凝土坝钻孔内平行布置2 条量程和精度均不同的监测仪;
所述的监测仪构成为:由多个传感器经加长杆串联而成,传感器分别为小量程高精度传感器和大量程传感器;
所述的小量程高精度传感器最大量程为0.5mm,精度为0.001mm;
所述的大量程传感器最大量程为5mm,精度为0.01mm;
所述小量程高精度传感器和大量程传感器外包裹包柔性泡沫管与混凝土隔离;
所述的加长杆外包PVC 材质的保护管以防止水泥浆粘结影响测量结果;
监测仪安装时,将每支传感器电缆集中后熔接成多芯电缆引出;
当监测仪安装埋设后,通过灌浆管回填水泥浆,达到龄期后即可进行裂缝监测。
2.一种混凝土大坝内部裂缝监测仪,其特征在于,所述的监测仪构成为:由多个传感器经加长杆串联而成,传感器分别为小量程高精度传感器和大量程传感器;
所述的小量程高精度传感器最大量程为0.5mm,精度为0.001mm;
所述的大量程传感器最大量程为5mm,精度为0.01mm;
所述小量程高精度传感器和大量程传感器外包裹包柔性泡沫管与混凝土隔离;
所述的加长杆外包PVC 材质的保护管以防止水泥浆粘结影响测量结果。