CN103112057A - 带天然木纹的重组木家具板及其制造方法 - Google Patents

带天然木纹的重组木家具板及其制造方法 Download PDF

Info

Publication number
CN103112057A
CN103112057A CN2013100754199A CN201310075419A CN103112057A CN 103112057 A CN103112057 A CN 103112057A CN 2013100754199 A CN2013100754199 A CN 2013100754199A CN 201310075419 A CN201310075419 A CN 201310075419A CN 103112057 A CN103112057 A CN 103112057A
Authority
CN
China
Prior art keywords
wood
wooden
wood grain
furniture
plates
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2013100754199A
Other languages
English (en)
Inventor
项兴君
解小聪
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Anhui Hongyi Bamboo Wood Science & Technology Co Ltd
Original Assignee
Anhui Hongyi Bamboo Wood Science & Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Anhui Hongyi Bamboo Wood Science & Technology Co Ltd filed Critical Anhui Hongyi Bamboo Wood Science & Technology Co Ltd
Priority to CN2013100754199A priority Critical patent/CN103112057A/zh
Publication of CN103112057A publication Critical patent/CN103112057A/zh
Pending legal-status Critical Current

Abstract

一种带天然木纹的重组木家具板及其制造方法,使用造价便宜、环保的速生材木皮为原料,木皮经过干燥,浸胶后干燥成待压木片,使用酚醛树脂或者聚胺酯粘合剂作为胶水。木皮层叠组坯,相邻二层的横向分布的木皮层和纵向分布的木皮层方向相互垂直以胶水粘合,用热压机或冷压机压制固化。固化后,家具板粗成品要平衡养生,然后抛光裁制成最终的尺寸。本发明具有天然实木的纹理,使用环保的速生材作为原料,美观,强度大,硬度高,造价便宜。

Description

带天然木纹的重组木家具板及其制造方法
技术领域
本发明新型涉及装饰材料领域,特别是涉及一种带天然木纹的重组木家具板及其制造方法。
背景技术
传统的家具板多数为人造板,材质主要为胶合板,刨花板,纤维板,还有部分使用竹板。全实木板由于价格昂贵已经很少使用了,即使用到也仅仅是薄板贴面,中间是其他材质的。目前市面上流行的人造板要么强度低,要么甲醛含量超标。竹板则容易起刺,而且价格没有优势。为了解决这个矛盾,如果能开发出带天然木纹的重组木家具板,利用其优秀的强度,硬度,不起刺,而同时有消费者能够接受的外观和材质,加上其相对低廉的价格,将能够完美的解决这个矛盾。
 
发明内容
为了克服上述现有技术的不足,本发明提供了一种带天然木纹的重组木家具板及其制造方法,它是由全实重组木做成的,具有天然木纹,造价便宜,原材料为环保的速生材,强度大,硬度高。
本发明所采用的技术方案是:使用造价便宜、环保的速生材木皮为原料,木皮经过干燥,浸胶后干燥成待压木片,使用酚醛树脂或者聚胺酯粘合剂作为胶水。木皮层叠组坯,相邻二层的横向分布的木皮层和纵向分布的木皮层方向相互垂直以胶水粘合,用热压机或冷压机压制固化。固化后,家具板粗成品要平衡养生,然后抛光裁制成最终的尺寸。
本发明的制造方法步骤如下:
步骤一:速生材刨成木皮;
步骤二:木皮经过阳光干燥或采选烘干机进行干燥,含水率控制在20%以内;
步骤三:浸胶后干燥成带待压木片;
步骤四:木皮层叠组坯,相邻二层的横向分布的木皮层和纵向分布的木皮层方向相互垂直以胶水粘合;
步骤五:用热压机或冷压机压制固化。固化后,家具板粗成品要平衡养生;
步骤六:抛光裁制成最终的尺寸。
所述胶水为酚醛树脂或者聚胺酯粘合剂。
本发明的有益效果是:具有天然实木的纹理,使用环保的速生材作为原料,美观,强度大,硬度高,造价便宜。
 
附图说明
图1为本发明的结构图。
图中,1-横向分布的木皮层,2-纵向分布的木皮层
具体实施方式
下面结合附图对本发明进行详细说明。
如图1所示,本发明所述的带天然木纹的重组木家具板及其制造方法,在生产开始阶段将刨切的杨木皮干燥,然后浸渍酚醛树脂。浸完胶后木皮经过干燥后在模具中按照相连的横向分布的木皮层1和纵向分布的木皮层2相互垂直排列组坯。经过热压机压制固化后得到重木板。将平衡后的重组木板修边抛光后得到天然木纹的家具板。
本发明的制造方法如下:
步骤一:速生材刨成木皮;
步骤二:木皮经过阳光干燥或采选烘干机进行干燥,含水率控制在20%以内;
步骤三:浸胶后干燥成带待压木片;
步骤四:木皮层叠组坯,相邻二层的横向分布的木皮层和纵向分布的木皮层方向相互垂直以胶水粘合;
步骤五:用热压机或冷压机压制固化。固化后,家具板粗成品要平衡养生;
步骤六:抛光裁制成最终的尺寸。
虽然本发明已以较佳实施例揭示如上,然其并非用以限定本发明,任何本领域技术人员,在不脱离本发明的精神和范围内,当可作些许的修改和完善,因此本发明的保护范围应当以权利要求书所界定的为准。

Claims (3)

1.一种带天然木纹的重组木家具板,其特征在于:木皮层叠组坯,相邻二层的横向分布的木皮层和纵向分布的木皮层方向相互垂直以胶水粘合。
2.一种带天然木纹的重组木家具板的制造方法,其特征在于:包括如下步骤:
步骤一:速生材刨成木皮;
步骤二:木皮经过阳光干燥或采选烘干机进行干燥,含水率控制在20%以内;
步骤三:浸胶后干燥成带待压木片;
步骤四:木皮层叠组坯,相邻二层的横向分布的木皮层和纵向分布的木皮层方向相互垂直以胶水粘合;
步骤五:用热压机或冷压机压制固化,固化后,家具板粗成品要平衡养生;
步骤六:抛光裁制成最终的尺寸。
3.如权利要求1或2所述的带天然木纹的重组木家具板及其制造方法,其特征在于:
所述胶水为酚醛树脂或者聚胺酯粘合剂。
CN2013100754199A 2013-03-11 2013-03-11 带天然木纹的重组木家具板及其制造方法 Pending CN103112057A (zh)