CN103063745B - 一种测量小径管内弧超声波声能损失的方法 - Google Patents
一种测量小径管内弧超声波声能损失的方法 Download PDFInfo
- Publication number
- CN103063745B CN103063745B CN201210590672.3A CN201210590672A CN103063745B CN 103063745 B CN103063745 B CN 103063745B CN 201210590672 A CN201210590672 A CN 201210590672A CN 103063745 B CN103063745 B CN 103063745B
- Authority
- CN
- China
- Prior art keywords
- small diameter
- diameter tube
- ultrasound wave
- inner arc
- wave
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
Description
Claims (1)