CN103008434A - 一种汽车外覆盖件模具废料切断工艺 - Google Patents
一种汽车外覆盖件模具废料切断工艺 Download PDFInfo
- Publication number
- CN103008434A CN103008434A CN2012105243829A CN201210524382A CN103008434A CN 103008434 A CN103008434 A CN 103008434A CN 2012105243829 A CN2012105243829 A CN 2012105243829A CN 201210524382 A CN201210524382 A CN 201210524382A CN 103008434 A CN103008434 A CN 103008434A
- Authority
- CN
- China
- Prior art keywords
- scrap
- cutting edge
- waste material
- cutoff
- deburring
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
本发明提供一种废料切断下滑容易,后续工序无变形,满足自动化连续生产的汽车外覆盖件模具废料切断工艺,关键在于上模刃口吃入在d1mm,废料下落Xmm,废料切断刀比下模刃口低d3=X+d1mm,且废料修边和废料切断刀切除废料分别在两个连续冲次完成,其中,d1为修边刃口吃入深度,X大于0并且小于可使模具闭合的最大高度。通过降低下模废料切断高度,在废料修边下滑后再在下一冲次切断,可以保证产品的表面质量,同时满足自动化连续生产的要求。
Description
一种汽车外覆盖件模具废料切断工艺
技术领域
[0001] 本发明涉及模具制造技术领域,具体涉及一种汽车外覆盖件模具废料切断工艺。背景技术
[0002] 汽车车身外覆盖件模具是汽车车身制造中要求最高、加工难度最大的模具,也是我国机电产品制造迅速发展的冷冲压工艺装备的一种。汽车车身覆盖件修边工艺的优劣,直接影响汽车外覆盖件的产品尺寸、表面质量和自动化生产顺利实施。当前趋势是为了节约成本,提倡节约化生产,模具工序数一减再减,现有模具工艺多数按照单工序修边考虑。对于传统的单工序模具修边及废料切断工艺,修边刃口 I吃入dl_ (—般为2_)将废料修掉,刃口侧废料下落3mm,废料切断刀比下模刃口低d2+dl=5mm,废料刀同时吃入d3mm(—般为2_)将其切断,因废料切断无压料芯压料,切断基本是撕裂状态,产生铁屑较多,且离制件型面近易带入模腔,造成后工序制件变形,另外如此紧凑的废料切断刀易造成卡料不下滑,影响自动化连续生产,如图1。
发明内容
[0003] 本发明的目的是提出一种废料切断下滑容易,后续工序无变形,满足自动化连续生产的汽车外覆盖件模具废料切断工艺。
[0004] 根据本发明提供的汽车外覆盖件模具废料切断工艺,关键在于上模刃口吃入dlmm,废料下落Xmm,废料切断刀比下模刃口低X+dlmm,且废料修边和废料切断刀切除废料分别在两个连续冲次完成,其中,dl为修边刃口吃入深度,X大于O并且小于可使模具闭合的最大闻度。
[0005] 本发明的汽车外覆盖件模具废料切断工艺,通过降低下模废料切断高度,在废料修边下滑后再在下一冲次切断,可以保证产品的表面质量,同时满足自动化连续生产的要求。
[0006] 废料修边后下落,由设置在废料切断刀前的挡料销挡住,再由废料切断刀切断。作为较佳的实施方式,废料由挡料销挡或储料槽暂存,在下一冲次再行切断,均可以实现本发明的目的。
[0007] 所述上模刃口设置在与上模座连接的上模修边镶块上,所述下模刃口设置在与下模座连接的下模修边镶块上。上下模刃口均是设置在修边镶块上,更换维修简单。
[0008] 所述下模废料切断刀有多组,这样可以同时多段切分废料。
附图说明
[0009]图1为传统汽车外覆盖件模具废料切断工艺结构示意图。
[0010]图2为本发明的汽车外覆盖件模具废料切断工艺结构示意图。
[0011] 图3为传统汽车外覆盖件模具废料切断工艺工作示意图。
[0012] 图4为本发明的汽车外覆盖件模具废料切断工艺工作示意图。具体实施方式
[0013] 下面对照附图,通过对实施实例的描述,对本发明的具体实施方式如所涉及的各构件的形状、构造、各部分之间的相互位置及连接关系、各部分的作用及工作原理等作进一步的详细说明。
[0014] 如图2,本发明的汽车外覆盖件模具废料切断工艺,相比图1和图3所示的传统工艺,上模刃口 I吃入dl=2謹,废料2下落Xmm,废料切断刀3比下模刃口 4低d3=X+2謹,且废料修边和废料切断刀3切除废料分别在两个连续冲次完成。其中,X值根据模具闭合高度允许的前提下合理选定。通过降低下模废料切断高度,在废料修边下滑后再在下一冲次切断,可以防止修边造成的铁屑带入模腔,保证产品的表面质量,同时满足自动化连续生产的要求。如图4,废料修边后下落,由设置在废料切断刀3前的挡料销5挡住,再由废料切断刀3切断。上下模废料切断刃口均是设置在上下模座上,更换维修简单。废料切断刀3可以有多组,这样可以同时多段切分废料。
Claims (4)
1. 一种汽车外覆盖件模具废料切断工艺,其特征在于上模刃口吃入dlmm,废料下落Xmm,废料切断刀比下模刃口低X+dlmm,且废料修边和废料切断刀切除废料分别在两个连续冲次完成,其中,dl为修边刃口吃入深度,X大于O并且小于可使模具闭合的最大高度。
2.根据权利要求1所述的汽车外覆盖件模具废料切断工艺,其特征在于废料修边后下落,由设置在废料切断刀前的挡料销挡住,再由废料切断刀切断。
3.根据权利要求1所述的汽车外覆盖件模具废料切断工艺,其特征在于所述上模刃口设置在与上模座连接的上模修边镶块上,所述下模刃口设置在与下模座连接的下模修边镶块上。
4.根据权利要求1或2或3所述的汽车外覆盖件模具废料切断工艺,其特征在于所述下模废料切断刀有多组。