CN102071640A - 一种桥梁伸缩缝装置的防水方法 - Google Patents

一种桥梁伸缩缝装置的防水方法 Download PDF

Info

Publication number
CN102071640A
CN102071640A CN2009102728239A CN200910272823A CN102071640A CN 102071640 A CN102071640 A CN 102071640A CN 2009102728239 A CN2009102728239 A CN 2009102728239A CN 200910272823 A CN200910272823 A CN 200910272823A CN 102071640 A CN102071640 A CN 102071640A
Authority
CN
China
Prior art keywords
waterproof
expansion joint
joint device
copper plate
neoprene
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2009102728239A
Other languages
English (en)
Inventor
刘祖江
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2009102728239A priority Critical patent/CN102071640A/zh
Publication of CN102071640A publication Critical patent/CN102071640A/zh
Pending legal-status Critical Current

Abstract

本发明是一种在桥梁上使用的伸缩缝装置的防水方法,要解决的是传统防水装置易损坏的问题。本发明是由两平行排列的T形型材1及T形型材之间的双组份聚氨酯密封胶2和氯丁橡胶3和铜板4和不绣钢压条5及镀锌锣栓6所构成。多年之后即使双组份聚氨酯密封胶受到损坏,而其下面的氯丁橡胶起到第二道防水的目的,如果氯丁橡胶受到损伤,最下层的紫铜板4就起到第三道防水的目的。由于这种层层设防的防水方法的实现,从而从根本上解决了伸缩缝装置长寿命防水的难题。附图是断面布置图。

Description

一种桥梁伸缩缝装置的防水方法 
技术领域:
建筑、采堀 
技术背景:
传统伸缩缝的防水方法不能达到桥梁设计要求 
发明内容:
本发明专利是一种在桥梁上使用的伸缩缝装置的防水方法,要解决的是传统防水装置易损坏的问题。 
本发明专利是由两平行排列的T形型材1及T形型材之间的双组份聚氨酯密封胶2和氯丁橡胶3和铜板4和不绣钢压条5及镀锌锣栓6所构成。 
聚氨酯密封胶2的物理特性:具有优良的耐磨性、低温柔软性、性能可调节范围较广、机械强度大、粘接性好、具有优良的复原性、耐油性能优良、耐生物老化、耐候性好,可适合于动态接缝。使用寿命可达15-20年。 
氯丁橡胶3的物理特性:属结晶型橡胶,强度、延伸率很好,接近天然橡胶的物理性能,拉伸强度一般可达到20MPa以上,伸长率可达600%以上,耐油性能相当于丙烯腈含量18左右的丁腈橡胶。氯丁橡胶是普通橡胶中的贵族。由于分子链中含氯原子,因而具有极性,在通用橡胶中,其极性仅次于丁腈橡胶。氯丁橡胶的物理机械性能和天然橡胶相似。其生胶具有很高的抗张强度和伸长率,属于自补强性橡胶。它的耐老化、耐热、耐油及耐化学腐蚀性比大然橡胶好。氯丁橡胶的耐老化性甚为优越,特别表现在耐大候及耐臭氧老化上。 
紫铜板4的物理特性;在所有属当中,紫铜板具有优良的抗挠性、在一定角度范围内、无数次地伸缩折挠而不断裂。 
利用上述三种物质的物理特性和机械性能,将它们有机的结合在一起,就能达到长寿命防水的目的。 
本发明专利实际上是一种桥梁伸缩缝装置的防水方法,是为了能彻底解决传统伸缩缝防水易脱落、寿命短的通病,其中7为C50钢纤维砼,8为锚固板,9为水平钢筋,10为桥梁梁台,11为桥面铺装,12为梁体预埋钢筋。 
具体操作方式: 
本防水方法在具体操作上有其非常特殊的一面,首先按伸缩缝各种规格设计预制不同宽度和厚度的氯丁橡胶3和紫铜板4,并在它们纵向两侧用专用模具冲出一定数量的锣丝眼,并在T形梁1的下竖板及不绣钢压条5上钻出与之对应锣丝眼,然后按图所示,用镀锌锣丝6依次将不绣钢压条5、紫铜板4、氯丁橡胶3、T形型材竖板紧紧拧紧,然后两T形型材拉伸至最大伸展位置,将现场调和的双组份聚氨脂密封2胶用注胶枪注入如图示位置并填满,儿天后聚氨脂密封胶就定型为一种非常有弹性的橡胶,在出厂安装时,根椐当时的温度用专用夹具调节两T形型钢之间的距离,由于双组份聚氨酯密封胶2是在两T形型材1之间距离最大的状态下预制的,将来无论什么状态,双组份聚氨酯密封胶2始终是处在受挤压状态,雨水是无法漏进去的,多年之后即使双组份聚氨酯密封胶受到损坏,而其下面的氯丁橡胶起到第二道防水的目的,如果氯丁橡胶受到损伤,最下层的紫铜板4就起到第三道防水的目的。由于这种层层设防的防水方法的实现,从而从根本上解决了伸缩缝装置长寿命防水的难题。
附图说明:附图是断面布置图 。 

Claims (1)

1.按伸缩缝各种规格设计预制不同宽度和厚度的氯丁橡胶3和紫铜板4,并在它们纵向两侧用专用模具冲出一定数量的锣丝眼,并在T形梁1的下竖板及不绣钢压条5上钻出与之对应锣丝眼,然后按图所示,用镀锌锣丝6依次将不綉钢压条5、紫铜板4、氯丁橡胶3、T形型材竖板紧紧拧紧,然后两T形型材拉伸至最大伸展位置,将现场调和的双组份聚氨脂密封2胶用注胶枪注入如图示位置并填满。
CN2009102728239A 2009-11-23 2009-11-23 一种桥梁伸缩缝装置的防水方法 Pending CN102071640A (zh)