CN101775533B - 高强、高韧性球墨铸铁及宽厚板工作辊 - Google Patents
高强、高韧性球墨铸铁及宽厚板工作辊 Download PDFInfo
- Publication number
- CN101775533B CN101775533B CN2010101120765A CN201010112076A CN101775533B CN 101775533 B CN101775533 B CN 101775533B CN 2010101120765 A CN2010101120765 A CN 2010101120765A CN 201010112076 A CN201010112076 A CN 201010112076A CN 101775533 B CN101775533 B CN 101775533B
- Authority
- CN
- China
- Prior art keywords
- cast iron
- strength
- iron
- working roll
- spheroidal graphite
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
Description
Claims (3)