CN101538918B - Method for refreshing ceramic tiles of exterior wall finish of building - Google Patents

Method for refreshing ceramic tiles of exterior wall finish of building Download PDF

Info

Publication number
CN101538918B
CN101538918B CN2008100244157A CN200810024415A CN101538918B CN 101538918 B CN101538918 B CN 101538918B CN 2008100244157 A CN2008100244157 A CN 2008100244157A CN 200810024415 A CN200810024415 A CN 200810024415A CN 101538918 B CN101538918 B CN 101538918B
Authority
CN
China
Prior art keywords
putty
ceramic tile
exterior wall
finish
roller coating
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN2008100244157A
Other languages
Chinese (zh)
Other versions
CN101538918A (en
Inventor
沈阳
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JIANGSU BAIDAI ENERGY-SAVING BUILDING MATERIALS Co.,Ltd.
Original Assignee
沈阳
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 沈阳 filed Critical 沈阳
Priority to CN2008100244157A priority Critical patent/CN101538918B/en
Publication of CN101538918A publication Critical patent/CN101538918A/en
Application granted granted Critical
Publication of CN101538918B publication Critical patent/CN101538918B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention relates to a method for refreshing ceramic tiles of an exterior wall finish of a building, which comprises five steps of cleaning a foundation course and filling in defects, scraping putty on ceramic tile surfaces, scraping and leveling putty, performing roller coating or spray coating of a primer, and performing roller coating or spray coating of a finish, wherein the excellent interlayer adhesion force can be formed by forming a permanent coating by the putty on the ceramic tile surfaces and old base surfaces of the ceramic tile surfaces and adopting the matching of the leveling putty and an elastic coating. The method overcomes the disadvantages of poor aesthetic property, and easy generation of stains and so on caused by adopting an interfacial agent to refresh the ceramic tiles of the exterior wall finish of the building in the prior art. The practice proves that the system has high safety factor, ensures that the outlines of the ceramic tiles cannot be seen after the finish is coated, can create rich and colorful decorative effect, and is particularly suitable for classical coating.

Description

A kind of method of refreshing ceramic tiles of exterior wall finish of building
(1) technical field:
The present invention relates to building decoration technology, particularly be directed against the method that phenomenons such as present ubiquitous exterior wall finish of building brick comes off, glazed layer cracking are carried out ceramic tile retreading.
(2) background technology:
Along with the development that the city makes rapid progress, modern architecture stands in great numbers.In order to make external surface of buildings attractive in appearance; People at the various face bricks of its external surface paving, except lithotomes such as paving granite, marble, more are paving glazed ceramic wall tile or mosaic usually; Because exposed wall facing brick has colourful decorative effect; And sturdy and durable, waterproof, be easy to clean, wear-resisting, color and luster stable, therefore, in the decoration of building, obtained using widely.But; Because through all the year round wind, Exposure to Sunlight, elemental destruction such as drench with rain, many old ceramic tiles, mosaic surface the part often occurs or large tracts of land comes off, the glazed layer cracking, take off porcelain; The long-term pollution thing accumulates the phenomenons such as decorative effect difference that cause, and can not adapt to the demand of modern city.Therefore, old ceramic tile face innovation is more and more.
Ceramic tile retreading is the engineering of coating, and what at first solve is putty and the adhesion stress problem of ceramic tile, mosaic glazed layer, in the prior art, adopts interfacial agents to carry out usually to refreshing ceramic tiles of exterior wall finish of building, and its concrete grammar is following: at first, clear up basic unit; Repair the ceramic tile place that comes off with cement mortar then, repair as far as possible and put down, treat the cement mortar bone dry after, smear whole exterior wall finish with liquid interfacial agents again.
The weak point of prior art is, though interfacial agents has adhesion stress preferably, smears the profile that still can find out ceramic tile behind the facing, and aesthetic property is poor.In addition, behind the use interfacial agents decorative constructure wall face, be prone to produce spot; Exterior wall finish intensity is not high.
(3) summary of the invention:
The present invention aims to provide the method for the refreshing ceramic tiles of exterior wall finish of building that a kind of aesthetic property is good, exterior wall finish intensity is high.
Technical solution of the present invention is following:
A kind of method of refreshing ceramic tiles of exterior wall finish of building may further comprise the steps,
1, the flat defective of cleaning basic unit and benefit:
Dust and the greasy dirt of removing the surface are clean; Remove attachment; Remove the soft part in surface; The hollowing position is excised; For crack or hollow sectors; Cut a hole " V " type with chisel; Repair with bouncing putty or cement mortar gradation; The thickest 2mm that is no more than of each repairing; Each repairing must be treated to carry out behind the last repairing bone dry (air drying is more than 8 hours, to guarantee its bone dry) again, mends flat until defective; All slits are filled and led up and non-loosening; Surfacing and the surface a little less than ceramic tile face 0.1-0.2cm, treat its bone dry after, carry out next procedure;
2, criticize ceramic tile face putty:
The mixed that ceramic tile face putty by specification is required also fully stirs into even no particle; (ceramic tile face putty is two component products not have the cream pasty state rubber cement that precipitates; Consist of lotion and powder) for use; Directly above-mentioned cream pasty state rubber cement is applied on last step repairing and the dried basal plane with spatula, consumption is controlled at 0.50kg/m 2In, after parching fully, completely criticize ceramic tile face putty again one time, consumption is at 0.8kg/m 2In, per pass is criticized and is coated with thickness and is no more than 0.6mm, and ceramic tile face putty parches (about 24 hours) fully, gets into next procedure;
3, criticize and scrape leveling putty:
(leveling putty is two component products with leveling putty; Consisting of lotion and powder) lotion and powder be by weight being 3.5~6: 1 mixed and fully stirring into even no particle; The cream pasty state that does not have deposition; Be applied over the cream pasty state leveling putty that stirs equably on the basal plane with spatula, THICKNESS CONTROL is in 2mm; Polishing after putty is done solid work, planeness require, and with the inspection of 2m guiding ruler, error is in 3mm, and no scratch and sand trace after parching fully, get into next procedure;
4, roller coating or spraying priming paint:
Leveling putty parches the even roller coating priming paint in back one time, parches back (about 6 hours) and gets into next process;
5, roller coating or spray paint:
After priming paint is done, roller coating or spray paint twice, following time roller coating or spray paint must parch afterwards (about 6 hours) at finish paint last time and construct,, no sag full, even to paint film, no color differnece.
The present invention is owing to adopt technique scheme, and the old basal plane of ceramic tile face putty and ceramic tile face forms permanent coating, and adopts leveling putty and the supporting ply adhesion that forms excellence of elastic coating.Ceramic tile face putty adhesion strength is high, and there are extremely strong adhesion stress in basic unit and other putty.Facts have proved that this system safety factor is high, supporting again other putty of use and priming paint, finish paint can be created colourful decorative effect, are particularly useful for classical application.Realized goal of the invention easily.
The major parameter of the inventive method:
Adhesion strength Mpa under the mark attitude Freeze thawing circulation adhesion strength Mpa Drying time (surface drying, h) Dry crack resistance of initial stage Alkali resistance (48h) Water resistance (96h)
1.0 0.47 ?3 Flawless No abnormal No abnormal
Further technical scheme is:
In the said step 2, when criticizing ceramic tile face putty, first pass is criticized should approach when being coated with and is criticized, and criticizes to criticize along the vertical direction when being coated with being coated with, and avoids ceramic tile face putty too much to stay in seam, after ceramic tile face putty parches (about 24 hours) fully, gets into next procedure.
(4) specific embodiment:
Embodiment 1, and the inventor has taked following method to the exterior wall finish of building construction of maintaining secrecy:
1) cleaning basic unit; Dust and the greasy dirt of removing the exterior wall finish surface are clean; Remove attachment; Remove the soft part in surface; With the excision of hollowing position,, cut a hole " V " type with chisel for crack or hollow sectors; The BD-333 bouncing putty gradation of using EMI to produce is repaired; The thickest 2mm that is no more than of each repairing, air drying carried out behind the bone dry more than 8 hours, until its surfacing; Defective is mended flat; All slits are filled and led up and non-loosening, and after the repairing, the surface is a little less than ceramic tile face 0.1cm; Metope after batch scraping is dry treat its bone dry more than 24 hours after, carry out next procedure;
2) criticize ceramic tile face putty: the BD-112 ceramic tile face putty of selecting for use EMI to produce, this putty are two component products, are lotion and powder (cement); Ratio by weight being 4: 1 is poured lotion and powder in the clean container into, fully stirs into even no particle, does not have the cream pasty state of deposition; Leave standstill and do to stir the back use after 10 minutes more slightly; Directly rubber cement is applied over basal plane with spatula, requires show-throughly, consumption is controlled at 0.50kg/m 2In, after parching fully, completely criticize ceramic tile face putty again one time, consumption is at 0.8kg/m 2In, should criticize being coated with for each batch when being coated with along the vertical direction, after ceramic tile face putty parched fully in 24 hours, get into next procedure;
3) criticize and scrape leveling putty: the lotion of the BD-110 leveling putty that EMI is produced and powder are by weight being fully to stir into even no particle at 3.5: 1; The cream pasty state that does not have deposition; Be applied over the leveling putty that stirs equably on the basal plane with spatula, THICKNESS CONTROL is in 2mm; Polishing after putty is done solid work, planeness require, and with the inspection of 2m guiding ruler, error is in 3mm, and no scratch and sand trace after parching fully, get into next procedure;
4) roller coating priming paint: leveling putty parch the back evenly roller coating Hangzhou method FilippoGammarelli coating Co., Ltd produce FW6501 alkali resistant priming paint one time, parch back (about 6 hours) and get into next process;
5) roller coating or spray paint: after priming paint is done, roller coating finish paint twice, following time roller coating last time finish paint parch afterwards (about 6 hours) and construct,, no sag full, even, no color differnece to paint film.
Embodiment 2, and the inventor has taked following method to the exterior wall finish of building construction of maintaining secrecy:
1) cleaning basic unit; Dust and the greasy dirt of removing the exterior wall finish surface are clean; Remove attachment; Remove the soft part in surface; With the excision of hollowing position,, cut a hole " V " type with chisel for crack or hollow sectors; The TB-998 putty gradation that marial rocks skill company produces in the use is repaired; The thickest 2mm that is no more than of each repairing, air drying was treated to carry out behind its bone dry in 8 hours, until its surfacing; Defective is mended flat; All slits are filled and led up and non-loosening, and after the repairing, the surface is a little less than ceramic tile face 0.2cm; Metope after batch scraping is dry treat its bone dry more than 24 hours after, carry out next procedure;
2) criticize ceramic tile face putty: the TBC-601 putty that will go up the production of marial rocks skill company (is similarly two component products; Consisting of lotion and powder) ratio that requires of by specification fully stirs into even no particle; The cream pasty state that does not have deposition; Leave standstill and do slightly after 10 minutes to stir the back use again, directly rubber cement is applied over basal plane with spatula, consumption is controlled at 0.50kg/m 2In, (requiring show-through) after parching fully in 12 hours, completely criticized ceramic tile face putty one time again, and consumption is at 0.8kg/m 2In, per pass is criticized and is coated with thickness and is no more than 0.6mm, criticizes along the vertical direction when being coated with for each batch being coated with, and after ceramic tile face putty parched fully in 24 hours, gets into next procedure;
3) criticize and scrape leveling putty: will go up the TBP-111 putty that marial rocks skill company produces and (be similarly two component products; Consist of lotion and powder) fully stir into even no particle in 4.5: 1 ratios; The cream pasty state that does not have precipitation; With spatula the putty that stirs is applied on the basal plane equably, THICKNESS CONTROL is in 2mm; Putty is done solid work back polishing, requires flatness with the inspection of 2m guiding ruler, error in 3mm, no scratch and sand trace;
4) spraying priming paint: putty parches the evenly roller coating Dalian ZB-06-9 alkali resistant seal coat one time that company of nation produces that shakes of back, parches back (after 6 hours) and gets into next process;
5) roller coating or spray paint: after priming paint is done, construction that roller coating finish paint twice, twice finish paint (parches the back) more than 6 hours at interval,, no sag full, even, no color differnece to paint film.
Embodiment 3, and the inventor has taked following method to the exterior wall finish of building construction of maintaining secrecy:
1) cleaning basic unit; Dust and the greasy dirt of removing the exterior wall finish surface are clean; Remove attachment; Remove the soft part in surface; With the excision of hollowing position,, cut a hole " V " type with chisel for crack or hollow sectors; Use the cement mortar gradation to repair; Each repair the thickest 2mm that is no more than, air drying carried out behind its bone dry guaranteeing more than 8 hours, until its surfacing; Defective is mended flat; All slits are filled and led up and non-loosening, and after the repairing, the surface is a little less than ceramic tile face 0.15cm; Metope after batch scraping is dry treat its bone dry more than 24 hours after, carry out next procedure;
2) criticize ceramic tile face putty: the BY-003 ceramic tile face putty that the rich Yun Yuebang company in Nanjing is produced (is similarly two component products; Consisting of lotion and powder) ratio that requires of by specification pours in the clean container; Fully stir into even no particle, do not have the cream pasty state of deposition, leave standstill and do slightly again after 10 minutes to use after the stirring; Directly rubber cement is applied over basal plane with spatula, consumption is controlled at 0.40kg/m 2, after parching fully in 12 hours, completely criticize ceramic tile face putty again one time, consumption is 0.7kg/m 2, after ceramic tile face putty parched fully in 24 hours, get into next procedure;
3) criticize and scrape leveling putty: the NP900 leveling putty with second own trade Co., Ltd in Shanghai produces is poured in the clean container in 6: 1 ratio; Fully stir into even no particle; The cream pasty state that does not have precipitation is applied over the putty that stirs on the basal plane with spatula equably, and THICKNESS CONTROL is in 2mm; Putty is done solid work back polishing, requires flatness with the inspection of 2m guiding ruler, error in 3mm, no scratch and sand trace;
4) roller coating priming paint: putty parches the evenly roller coating Dalian outer wall paint of ZB-08-701 wall prestige one time that company of nation produces that shakes of back, parches back (after 6 hours) and gets into next process;
5) roller coating or spray paint: after priming paint is done, construction that roller coating finish paint twice, twice finish paint (parches the back) more than 6 hours at interval,, no sag full, even, no color differnece to paint film.
The present invention is owing to adopt technique scheme, and the old basal plane of ceramic tile face putty and ceramic tile face forms permanent coating, and adopts general leveling putty and the supporting ply adhesion that forms excellence of elastic coating.Facts have proved that this system safety factor is high, supporting again other putty of use and priming paint, finish paint are smeared the profile of not seeing ceramic tile behind the facing, can create colourful decorative effect, are particularly useful for classical application.Realized goal of the invention easily.
Certainly, under inventive concept of the present invention, the present invention has multiple form of implementation, and those skilled in the art read and need not pay creative work behind this manual and can reveal again, have not just detailed at this.

Claims (2)

1. the method for a refreshing ceramic tiles of exterior wall finish of building may further comprise the steps,
1) the flat defective of cleaning basic unit and benefit: dust and the greasy dirt of removing the exterior wall finish surface are clean; Remove attachment; Remove the soft part in surface; The hollowing position is excised; For crack or hollow sectors; Cut a hole " V " type with chisel; Repair with bouncing putty or cement mortar gradation; The thickest 2mm that is no more than of each repairing, each repairing must be treated to carry out behind the last repairing bone dry again, mends until defective and puts down; All slits are filled and led up and non-loosening; Surfacing and the surface a little less than ceramic tile face 0.1-0.2cm, treat its bone dry after, carry out next procedure;
2) criticize ceramic tile face putty: with ceramic tile face putty lotion and powder; The mixed that by specification requires also fully stirs into even no particle; The cream pasty state rubber cement that does not have deposition is for use; Directly above-mentioned cream pasty state rubber cement is applied on last step repairing and the dried basal plane with spatula, consumption is controlled at 0.50kg/m 2In, after parching fully, completely criticize ceramic tile face putty again one time, consumption is at 0.8kg/m 2In, per pass is criticized and is coated with thickness and is no more than 0.6mm, after ceramic tile face putty parches fully, gets into next procedure;
3) criticize and scrape leveling putty: with leveling putty lotion and powder by weight being 3.5~6: 1 mixed and fully stirring into even no particle; The cream pasty state that does not have deposition; Be applied over the leveling putty that stirs equably on the basal plane with spatula, THICKNESS CONTROL is in 2mm; Polishing after putty is done solid work, planeness require, and with the inspection of 2m guiding ruler, error is in 3mm, and no scratch and sand trace after parching fully, get into next procedure;
4) roller coating or spraying priming paint: leveling putty parches the even roller coating in back or sprays priming paint one time, parches the back and gets into next process;
5) roller coating or spray paint: after priming paint is done, roller coating or spray paint twice, following time roller coating or spray paint must parch afterwards at finish paint last time and constructing,, no sag full, even to paint film, no color differnece.
2. the method for a kind of refreshing ceramic tiles of exterior wall finish of building according to claim 1 is characterized in that: in said step 2, criticize to criticize along the vertical direction when being coated with being coated with, after ceramic tile face putty parches fully, get into next procedure.
CN2008100244157A 2008-03-21 2008-03-21 Method for refreshing ceramic tiles of exterior wall finish of building Active CN101538918B (en)