CN101497511A - 环保轻质混凝土 - Google Patents
环保轻质混凝土 Download PDFInfo
- Publication number
- CN101497511A CN101497511A CNA2008100334825A CN200810033482A CN101497511A CN 101497511 A CN101497511 A CN 101497511A CN A2008100334825 A CNA2008100334825 A CN A2008100334825A CN 200810033482 A CN200810033482 A CN 200810033482A CN 101497511 A CN101497511 A CN 101497511A
- Authority
- CN
- China
- Prior art keywords
- pellet
- environment friendly
- foaming
- cement slurry
- mixed
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明是关于建筑轻质混凝土材料领域的,特别为一种环保轻质混凝土,其配料是环保混合发泡粒料、泡沫水泥浆料、混合发泡搅拌装置,一次快速发泡成混凝土浆,该环保混合发泡粒料为;废弃混凝土加气发泡砌块粉碎粒料、淤泥烧结陶粒,混合干料体积密度为400公斤/立方米左右,直径在5毫米~20毫米。本发明的目的是再造一种轻质、保温、耐火、高强度、一定程度增加了型韧性,而且是全新意义上的环保轻质混凝土。
Description
技述领域
本发明是关于建筑轻质混凝土材料领域的,特别为一种环保轻质混凝土。
背景技术
现在的建筑为了达到节能保温要求;采用混凝土加气发泡砌块、或水泥基发泡制品构筑墙体,当墙体需要装修拆除时,遗弃大量加气发泡砌块,由于发泡砌块体积较大,当垃圾处理时、运输成本很大,总之该固体废料给城市造成很大的环保压力,同时也不符合资源最大化利用,并且这种问题在未来将更加突出。
实用新型内容
本发明的目的是利用上述材料为主料;再造一种轻质、保温、耐火、高强度、且是全新意义上的环保轻质混凝土。
本发明的目的是通过下述技术方案予以实现:
首先将废弃混凝土加气发泡砌块粉碎成直径在5毫米~20毫米粒料、淤泥烧结陶粒、预拌混合,泡沫水泥浆料,混合发泡搅拌装置,一次快速发泡成混凝土浆料,施工现场实施浇注,适当振动,48小时以上凝固期即可。
具体实施方式
下面结合物料施例对发明实进一步描述;
混合发泡颗粒,重量比例百分比为;
废弃加气砌块砖粉碎颗粒50%左右
淤泥烧结陶粒50%左右
总容量为100%,干料体积密度为400公斤/立方米左右,
环保轻质混凝土主要料,重量比例百分比为;
环保混合发泡粒料50%左右
泡沫水泥浆料40%左右
总容量为100%,干料体积密度为400~1000公斤/立方米左右
本发明的有益效果是:
1适合墙面和地面的灌模施工,大规模施工方便,废弃资源最大化利用;
2环保节能,轻质,保温,耐火,可承重,成本低,不易变形。
Claims (7)
1 环保轻质混凝土,其特征在于环保混合发泡粒料、泡沫水泥浆料,混合发泡搅拌装置,一次快速发泡成混凝土浆料。
2 根据权利要求1所述的环保轻质混凝土,其特征在于所述的环保混合发泡粒料为;废弃混凝土加气发泡砌块粉碎粒料、淤泥烧结陶粒,混合干料体积密度为400公斤/立方米左右,直径在5毫米~20毫米。
3 根据权利要求1、2所述的环保轻质混凝土,其特征在于所述的泡沫水泥浆料主要料为;水、水泥发泡剂、水泥。
4 根据权利要求1、3所述的环保轻质混凝土,其特征在于所述的发泡混合搅拌装置为;适合搅拌粒料的发泡、混合功能电动设备。
5 根据权利要求1所述的环保轻质混凝土,其特征在于所述的混合发泡粒料、与发泡水泥浆料、重量比例百分比为;
环保混合发泡粒料50%左右
泡沫水泥浆料50%左右
总容量为100%,
干料体积密度为400~1000公斤/立方米左右
6 根据权利要求1所述的环保轻质混凝土,其特征在于所述的混合发泡粒料、与发泡水泥浆料、重量比例百分比为;
环保混合发泡粒料35%左右
泡沫水泥浆料65%左右
总容量为100%,
干料体积密度为400~1000公斤/立方米左右
7 根据权利要求1所述的环保轻质混凝土,其特征在于所述的混合发泡粒料、与发泡水泥浆料、重量比例百分比为;
环保混合发泡粒料65%左右
泡沫水泥浆料35%左右
总容量为100%,
干料体积密度为400~1000公斤/立方米左右