CN101433955A - Method and apparatus for casting zinc-base alloy ingot - Google Patents
Method and apparatus for casting zinc-base alloy ingot Download PDFInfo
- Publication number
- CN101433955A CN101433955A CNA2008101439561A CN200810143956A CN101433955A CN 101433955 A CN101433955 A CN 101433955A CN A2008101439561 A CNA2008101439561 A CN A2008101439561A CN 200810143956 A CN200810143956 A CN 200810143956A CN 101433955 A CN101433955 A CN 101433955A
- Authority
- CN
- China
- Prior art keywords
- cooling water
- zinc
- water
- base alloy
- ingot
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention relates to a method and a device for casting a zinc based alloy ingot. The method comprises the following steps: firstly molten metal is cast in an ingot mould, during the solidification, the surface of the ingot is cooled down through spraying cooling water, and the flow rate of the cooling water is between 200 and 20,000g/m. The device comprises a linear moulding machine comprising a plurality of casting moulds making the rectilinear motion and moulds arranged in the casting moulds; the device is characterized in that the device also comprises a spraying device spraying the cooling water on the ingots in the cast moulds one by one, the spraying device consists of a spray head, a circulating cooling water pipe and an open water tank receiving the cooling water, and the spraying device can be an atomization spraying device. In the method, through spraying the cooling water, the upper surface of the zinc based alloy ingot is quickly shrunk, and the central part of fused mass is quickly solidified, thereby avoiding the shrinkage hole phenomenon; moreover, by limiting the flow rate of the cooling water, the formation of dent on the ingot surface due to the direct impact of the cooling water is avoided.
Description
Technical field
The present invention relates to a kind of production method and device of zinc-containing alloy, particularly a kind of casting method of zinc-base alloy ingot and device.
Background technology
The production method of casting zinc ingot metal and ZINC ALLOY generally is earlier Metal Melting to be changed into liquid at present, and motlten metal liquid is cast in the mould, has to adopt the mode of artificial cooling or cooling naturally to make it be frozen into the solid ingot of required form again.Because in the motlten metal process of setting, the temperature difference reaches 400 degree, in this temperature-fall period, according to principle of expanding with heat and contracting with cold, the ingot volume will inevitably be greater than cooled ingot volume when finishing in casting, and for the less strip ingot of volume, the cooling velocity at its ingot edge is faster than the cooling velocity at ingot center, volume compensation in its shrinkage process is concentrated to the upper surface at ingot center, forms surperficial shrinkage cavity.As adopt the artificial type of cooling such as direct pouring cooling water, can quicken the cooling velocity at ingot center, avoid forming surperficial shrinkage cavity because of the margin and center setting rate of upper surface is inconsistent, the artificial type of cooling commonly used has: 1, mold is placed in the tank, 2, to mold bottom water spray, 3, to the direct trickle of ingot surface.The third mode is a usual way, but there is weak point in it, and promptly easy upper surface at zinc-base alloy ingot forms indenture because of current directly impact.Its reason is: prior art does not limit the flow velocity of cooling water usually, flows through by force as water, then can produce strong impulsive force, and this moment, its alloy pig of zinc was just finished the casting program, the surface ot-yet-hardened, under strong excessively water impact, the surface can produce deformation and form indenture.No matter be surperficial shrinkage cavity or indenture, all can influence the surface quality of zinc-base alloy ingot, make product not meet the physical specification test stone.
Therefore, the casting method of existing zinc-base alloy ingot and device need further to improve.
Summary of the invention
The object of the present invention is to provide a kind of casting method of zinc-base alloy ingot, it can eliminate the surperficial shrinkage cavity and the indenture of zinc ingot metal, makes the surface quality of zinc-base alloy ingot meet the physical specification test stone of product.
The object of the present invention is to provide a kind of pouring device of zinc-base alloy ingot, it realizes said method, realizes eliminating the surperficial shrinkage cavity of zinc ingot metal and the effect of indenture.
Technical scheme of the present invention is:
A kind of casting method of zinc-base alloy ingot, it is after being cast to motlten metal in the ingot mould tool earlier, spraying cooling water being carried out on the surface of the ingot in the process of setting cool off, it is characterized in that: the flow velocity of described cooling water is 300~20000 Grams Per Minutes.
As to further improvement of the present invention, described cooling water is the atomizing cooling water, and the flow velocity of described atomizing cooling water is 200~1000 Grams Per Minutes.
A kind of pouring device of zinc-base alloy ingot; it comprises the straight line moulding machine; described straight line moulding machine comprises a plurality of straight-line molds and places the interior mould of each mold; it is characterized in that: it also comprises the spray equipment that the ingot in the mould after the casting is carried out one by one spraying cooling water, and the flow velocity of described cooling water is 300~20000 Grams Per Minutes.
As to further improvement of the present invention, described spray equipment is made up of shower nozzle, circulating cooling water pipe and the uncovered water tank of accepting cooling water, and described shower nozzle is fixedly set in the top of straight line moulding machine, and described water tank places straight line machine mold below.
As to further improvement of the present invention, described spray equipment is an atomizing sprayer, and described shower nozzle is an atomizer, and the flow velocity of described atomizing cooling water is 200~1000 Grams Per Minutes.
As to further improvement of the present invention, the vertical range of described shower nozzle and mold is 20~40 centimetres.
As to further improvement of the present invention, the lower surface of described mold places the cooling water in the uncovered water tank.
As to further improvement of the present invention, described spray equipment also comprises the cooling tower that connects, makes water quench in the water tank with tank pipe, and described cooling tower outlet is connected with the water pump that connects with pipe-line.
As to further improvement of the present invention, also be provided with hot-tub between described water tank and the cooling tower, also be provided with the cooling pond between described cooling tower outlet and the water pump.
The invention has the beneficial effects as follows:
1, the present invention can be according to the shape and the size decision cooling water flow velocity of zinc-containing alloy kind, ingot, and with the drift limit of cooling water in 200~1000 Grams Per Minutes, can avoid current that ingot surface was formed strong impulsive force, both reach the effect of accelerating ingot center cooling velocity, and avoided ingot surface to form indenture again.
2, the present invention also provides the type of cooling to the spray of the zinc-base alloy ingot after casting atomizing cooling water, and the flow velocity of qualification atomizing cooling water is 200~1000 Grams Per Minutes.It is when guaranteeing cooling effect, and no current directly impact ingot surface, has fundamentally eliminated the influence factor of indenture formation, avoids forming indenture, the surface of gained zinc-base alloy ingot product bright and clean smooth.
3, it is selective that device of the present invention can provide the multiple type of cooling, as cool water shower device, atomizing cool water shower device, these two kinds of different types of cooling only need can realize by selecting different shower nozzles, the above-mentioned type of cooling can also place the mode of cooling off in the uncovered water tank in conjunction with the mold lower surface, mode that also can the configuration cycles cooling water, these modes can make cooling effect better, and product surface quality is better.
The invention will be further described below in conjunction with accompanying drawing:
Description of drawings
Fig. 1 is the structural representation of apparatus of the present invention.
Among the figure: 1-mould, 2-ingot, 3-spray equipment, 4-water pipe, 5-water supply pump, 6-water cooling pond, 7-cooling tower, 8-heat-exchanger pump, 9-hot-tub, 10-straight line moulding machine, 11-water tank.
The specific embodiment
Embodiment 1:
A kind of casting method of zinc-base alloy ingot, it is used to the zinc-base alloy ingot of casting, and it is after being cast to motlten metal in the ingot mould tool earlier, spraying cooling water being carried out on the surface of the ingot in the process of setting cool off, and the flow velocity of cooling water is 20000 Grams Per Minutes.
A kind of pouring device of zinc-base alloy ingot; as shown in Figure 1; it comprises straight line moulding machine 10; straight line moulding machine 10 comprises a plurality of straight-line molds and places the interior mould 1 of each mold; it also comprises the spray equipment that the ingot in the mould after the casting 1 is carried out one by one spraying cooling water; spray equipment is by shower nozzle 3; circulating cooling water pipe 4 is formed with the uncovered water tank 11 of accepting cooling water; shower nozzle 3 is fixedly set in the top of straight line moulding machine 10; the flow velocity of the cooling water that shower nozzle 3 is sprayed is 20000 Grams Per Minutes; water tank 11 places straight line moulding machine 10 belows; shower nozzle 3 is 40 centimetres with the vertical range of mold; the lower surface of mold places the cooling water in the uncovered water tank 11; spray equipment also comprises with water tank 11 and being connected by pipeline; make the cooling tower 7 of water quench in the water tank 11, cooling tower 7 outlets are connected with the water supply pump 5 that connects with shower nozzle 3 pipelines.Water tank 11 links to each other with hot-tub 9, and the water in the hot-tub 9 is delivered to cooling tower 7 by heat-exchanger pump 8, and cooling tower 7 outlets link to each other with water cooling pond 6, and water supply pump 5 links to each other with spray equipment.
Embodiment 2:
A kind of casting method of zinc-base alloy ingot, it is used to the zinc-base alloy ingot of casting, and it is after being cast to motlten metal in the ingot mould tool earlier, spraying cooling water being carried out on the surface of the ingot in the process of setting cool off, and the flow velocity of cooling water is 1100 Grams Per Minutes.
A kind of pouring device of zinc-base alloy ingot; as shown in Figure 1; it comprises straight line moulding machine 10; straight line moulding machine 10 comprises a plurality of straight-line molds and places the interior mould 1 of each mold; it also comprises the spray equipment that the ingot in the mould after the casting 1 is carried out one by one spraying cooling water; spray equipment is by shower nozzle 3; circulating cooling water pipe 4 is formed with the uncovered water tank 11 of accepting cooling water; shower nozzle 3 is fixedly set in the top of straight line moulding machine 10; the flow velocity of the cooling water that shower nozzle 3 is sprayed is 1100 Grams Per Minutes; water tank 11 places straight line moulding machine 10 belows; shower nozzle 3 is 20 centimetres with the vertical range of mold; the lower surface of mold places the cooling water in the uncovered water tank 11; spray equipment also comprises with water tank 11 and being connected by pipeline; make the cooling tower 7 of water quench in the water tank 11, cooling tower 7 outlets are connected with the water supply pump 5 that connects with shower nozzle 3 pipelines.Water tank 11 links to each other with hot-tub 9, and the water in the hot-tub 9 is delivered to cooling tower 7 by heat-exchanger pump 8, and cooling tower 7 outlets link to each other with water cooling pond 6, and water supply pump 5 links to each other with spray equipment.
Embodiment 3:
A kind of casting method of zinc-base alloy ingot, it is after being cast to motlten metal in the ingot mould tool earlier, spraying cooling water being carried out on the surface of the ingot in the process of setting cool off, and cooling water is the atomizing cooling water, and the flow velocity of atomizing cooling water is 200 Grams Per Minutes.
A kind of pouring device of zinc-base alloy ingot; as shown in Figure 1; it comprises straight line moulding machine 10; straight line moulding machine 10 comprises a plurality of straight-line molds and places the interior mould 1 of each mold; it also comprises the spray equipment that the ingot in the mould after the casting 1 is carried out one by one spraying cooling water; spray equipment is made up of shower nozzle 3, circulating cooling water pipe 4 and the uncovered water tank 11 of accepting cooling water; shower nozzle 3 is fixedly set in the top of straight line moulding machine 10; spray equipment is an atomizing sprayer; shower nozzle 3 is an atomizer, and the flow velocity of atomizing cooling water is 200 Grams Per Minutes.Water tank 11 places straight line moulding machine 10 belows; shower nozzle 3 is 30 centimetres with the vertical range of mold; the lower surface of mold places the cooling water in the uncovered water tank 11; spray equipment comprises also with water tank 11 and connects, makes the cooling tower 7 of water quench in the water tank 11 by pipeline that cooling tower 7 outlets are connected with the water supply pump 5 that connects with shower nozzle 3 pipelines.Water tank 11 links to each other with hot-tub 9, and the water in the hot-tub 9 is delivered to cooling tower 7 by heat-exchanger pump 8, and cooling tower 7 outlets link to each other with water cooling pond 6, and water supply pump 5 links to each other with spray equipment.
Embodiment 4:
A kind of casting method of zinc-base alloy ingot, it is after being cast to motlten metal in the ingot mould tool earlier, spraying cooling water being carried out on the surface of the ingot in the process of setting cool off, and cooling water is the atomizing cooling water, and the flow velocity of atomizing cooling water is 1000 Grams Per Minutes.
A kind of pouring device of zinc-base alloy ingot; as shown in Figure 1; it comprises straight line moulding machine 10; straight line moulding machine 10 comprises a plurality of straight-line molds and places the interior mould 1 of each mold; it also comprises the spray equipment that the ingot in the mould after the casting 1 is carried out one by one spraying cooling water; spray equipment is made up of shower nozzle 3, circulating cooling water pipe 4 and the uncovered water tank 11 of accepting cooling water; shower nozzle 3 is fixedly set in the top of straight line moulding machine 10; spray equipment is an atomizing sprayer; shower nozzle 3 is an atomizer, and the flow velocity of atomizing cooling water is 1000 Grams Per Minutes.Water tank 11 places straight line moulding machine 10 belows; shower nozzle 3 is 30 centimetres with the vertical range of mold; the lower surface of mold places the cooling water in the uncovered water tank 11; spray equipment comprises also with water tank 11 and connects, makes the cooling tower 7 of water quench in the water tank 11 by pipeline that cooling tower 7 outlets are connected with the water supply pump 5 that connects with shower nozzle 3 pipelines.Water tank 11 links to each other with hot-tub 9, and the water in the hot-tub 9 is delivered to cooling tower 7 by heat-exchanger pump 8, and cooling tower 7 outlets link to each other with water cooling pond 6, and water supply pump 5 links to each other with spray equipment.
Claims (9)
1, a kind of casting method of zinc-base alloy ingot, it is after being cast to motlten metal in the ingot mould tool earlier, spraying cooling water being carried out on the surface of the ingot in the process of setting cool off, it is characterized in that: the flow velocity of described cooling water is 300~20000 Grams Per Minutes.
2, the casting method of zinc-base alloy ingot according to claim 1 is characterized in that: described cooling water is the atomizing cooling water, and the flow velocity of described atomizing cooling water is 200~1000 Grams Per Minutes.
3, a kind of pouring device of zinc-base alloy ingot; it comprises the straight line moulding machine; described straight line moulding machine comprises a plurality of straight-line molds and places the interior mould of each mold; it is characterized in that: it also comprises the spray equipment that the ingot in the mould after the casting is carried out one by one spraying cooling water, and the flow velocity of described cooling water is 300~20000 Grams Per Minutes.
4, the pouring device of zinc-base alloy ingot according to claim 3; it is characterized in that: described spray equipment is made up of shower nozzle, circulating cooling water pipe and the uncovered water tank of accepting cooling water; described shower nozzle is fixedly set in the top of straight line moulding machine, and described water tank places straight line machine mold below.
5, the pouring device of zinc-base alloy ingot according to claim 3 is characterized in that: described spray equipment is an atomizing sprayer, and described shower nozzle is an atomizer, and the flow velocity of described atomizing cooling water is 200~1000 Grams Per Minutes.
6, the pouring device of zinc-base alloy ingot according to claim 3 is characterized in that: the vertical range of described shower nozzle and mold is 20~40 centimetres.
7, the pouring device of zinc-base alloy ingot according to claim 3 is characterized in that: the lower surface of described mold places the cooling water in the uncovered water tank.
8, according to the pouring device of each described zinc-base alloy ingot of claim 3~7, it is characterized in that: described spray equipment also comprises the cooling tower that connects, makes water quench in the water tank with tank pipe, and described cooling tower outlet is connected with the water pump that connects with pipe-line.
9, the pouring device of zinc-base alloy ingot according to claim 8 is characterized in that: also be provided with hot-tub between described water tank and the cooling tower, also be provided with the cooling pond between described cooling tower outlet and the water pump.